Physical Properties Metric English Comments
Melt Flow 9.00 - 14.0 g/10 min

@Load 1.10 kg,
Temperature 300 °C
9.00 - 14.0 g/10 min

@Load 2.43 lb,
Temperature 572 °F
ASTM D1238
Oxford Polymers PC 714-FR Series PC, Flame retardant
Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial..
Melt Flow 9.00 - 18.0 g/10 min
9.00 - 18.0 g/10 min
Average value: 13.7 g/10 min Grade Count:3
Overview of materials for Liquid Crystal Polymer (LCP), Unfilled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Unfilled". Each property range of values reported is minimum and maximum v..
Melt Flow 9.00 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.00 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 1079E Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 9.00 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.00 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 1097D Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinpolene TPP1040 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 40% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection ..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Synres® PP G10 17 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Synres® PP G20 62 Polypropylene, Glass Reinforced
Notes: The Specialty Compounding Division offers a proprietary line of glass reinforced polypropylene. Typical applications include automotive, building and construction, industrial as well as many ..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1155A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1183A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® TL-1273A Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 175 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 347 °F
ASTM D1238
Teknor Apex Telcar® TL-2069B Thermoplastic Elastomer
Uses: Caps; Food Packaging; Liners Pellets Processing Method: Extrusion; Injection Molding; Press Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmIn..
Melt Flow 9.00 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.00 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron KU602 ABS Heat Resistant
High ImpactInformation provided by Bhansali
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinpolene CPP2040 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati..
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinpolene FRF2074 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Flame Retardant Uses: Appliance Components; Housings Forms: PelletsInformation Provided by Teknor Apex
Melt Flow 9.00 g/10 min

@Load 2.16 kg,
Temperature 230 °C
9.00 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinpolene TPP1030 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 30% Filler by Weight Uses: Automotive Applications; Housings Forms: Pellets Processing Method: Injection ..
Melt Flow 9.00 - 22.0 g/10 min
9.00 - 22.0 g/10 min
Average value: 16.4 g/10 min Grade Count:8
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Melt Flow 9.00 - 15.0 g/10 min
9.00 - 15.0 g/10 min
Average value: 12.0 g/10 min Grade Count:4
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum..
Melt Flow 9.00 - 110 g/10 min
9.00 - 110 g/10 min
Average value: 54.6 g/10 min Grade Count:7
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..
Melt Flow 9.00 g/10 min

@Load 10.0 kg,
Temperature 220 °C
9.00 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Bhansali Engineering Abstron KU602 ABS Heat Resistant
High ImpactInformation provided by Bhansali