Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D123 |
Niche Polymer PPCM15BK Copolymer PP Information provided by Niche Polymer |
|||
Melt Flow | 15.0 g/10 min | 15.0 g/10 min | ASTM D123 |
Niche Polymer PPHM15BK Homopolymer PP Information provided by Niche Polymer |
|||
Melt Flow | 15.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
15.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex HFFR 2005PC Polyolefin, Halogen Free RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable JacketingAgency Ratings: IEC Unspecified Rating; ICEA Unspecifie.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 125 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 257 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1023 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1488A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1782 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
15.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1829-R Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1881B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1959G Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
15.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2242 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2287M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
15.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2375A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2664B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 - 50.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
15.0 - 50.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB1511 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 15.0 - 45.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
15.0 - 45.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB3462 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Uses: Non-specific Food Applications Forms: Pellets Pro.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW001LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (300000 ppm) Filler/Reinforcement: Calcium Carbonate Filler Uses: Film Forms: Pelle.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1791 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Uses: Film; Sheet Forms: Pellets Processing Method: Injection Molding;.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4945A Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4985F Thermoplastic Elastomer Notes: Telcar OBC has superior mechanical strength and higher elongation which will provide a tougher more durable finished product. Telcar OBC can be used in less demanding sealing applications. T.. |
|||
Melt Flow | 15.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
15.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1420C Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injecti.. |
|||
Melt Flow | 15.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
15.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2460A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 175 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 347 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2590F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 15.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
15.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron HR60N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Melt Flow | 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2890M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 15.0 - 100 g/10 min | 15.0 - 100 g/10 min | Average value: 61.0 g/10 min Grade Count:5 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Melt Flow | 15.0 - 16.3 g/10 min | 15.0 - 16.3 g/10 min | Average value: 15.9 g/10 min Grade Count:3 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |