Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 110 g/10 min @Load 2.16 kg, Temperature 180 °C |
110 g/10 min @Load 4.76 lb, Temperature 356 °F |
|
Hybrid Plastics Polyamide POSS® Flow Masterbatch POSS® Flow masterbatches show success in reducing the melt viscosity of a variety of injection molded and extruded resins. Hybrid Plastics now introduces such a solution for polyamide polymers. P.. |
|||
Melt Flow | 110 g/10 min | 110 g/10 min | ASTM D1238 |
Flint Hills P9H9Z-018 Polypropylene Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Melt Flow | 110 g/10 min @Load 10.0 kg, Temperature 400 °C |
110 g/10 min @Load 22.0 lb, Temperature 752 °F |
|
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Melt Flow | 110 g/10 min @Load 2.16 kg, Temperature 230 °C |
110 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RJ900MO Polypropylene Random Copolymer RJ900MO is a polypropylene random copolymer with high melt flow and good transparency. Products originating from this grade have excellent transparency and gloss, and good balance of stiffness and .. |
|||
Melt Flow | 110 g/10 min @Load 2.16 kg, Temperature 230 °C |
110 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding Lumicene® MR110MC2 is a metallocene random copolymer with a melt flow index of 110 g/10 min for injection molding. This Lumicene® MR110MC2 high fluidity differs from standard random copolymers by .. |
|||
Melt Flow | 110 g/10 min @Load 5.00 kg, Temperature 260 °C |
110 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a.. |
|||
Melt Flow | 110 g/10 min @Load 2.16 kg, Temperature 230 °C |
110 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TI2900C High Crystallinity Copolymer Polypropylene Description: Highly Crystalline Homopolymer Phase, Very High Molecular Weight EPR Phase, Very High Flexural Modulus, Reduced Emissions, Reduced Gels.Applications: Suggested uses include compounding... |
|||
Melt Flow | 110 g/10 min @Load 5.00 kg, Temperature 275 °C |
110 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Transparent up to maximum 2.5 mm.Tarnamid® has the following main properties.. |
|||
Melt Flow | 110 g/10 min @Load 10.0 kg, Temperature 275 °C |
110 g/10 min @Load 22.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET |
|||
Melt Flow | 110 g/10 min @Load 5.00 kg, Temperature 266 °C |
110 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East) VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin. |