Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.0 g/10 min @Load 1.00 kg, Temperature 235 °C |
10.0 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Teknor Apex Chemlon® 100 L Nylon 66, Unreinforced Notes: Internally and externally lubricated; General Purpose; Double-lubricated for improved part ejection and machine feed Processing Method: Injection Molding Forms: PelletsInformation Provided by.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 125 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 257 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 2313 Thermoplastic Elastomer Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly.. |
|||
Melt Flow | 10.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1650L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1698 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 125 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 257 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1900 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2775 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 10.0 kg, Temperature 190 °C |
10.0 - 30.0 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB0051 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW008LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Filler/Reinforcement: Calcium Carbonate Filler Uses: Film Forms: Pelle.. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 - 30.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW5335 Specialty Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (200000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 10.0 - 30.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 - 30.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW5365 Specialty Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (500000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor .. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Sinpolene TPP2010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1269A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2503S Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2519E Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2683A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-CC40 Natural Copolymer Polypropylene, 40% Calcium Carbonate Filled Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-GF25 Natural Impact Polypropylene, 25% Glass Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPH-CC40 Natural Homopolymer Polypropylene, 40% Calcium Carbonate Filled Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPH-GF10 Natural Homopolymer Polypropylene, 10% Glass Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPH-GF40 Natural Homopolymer Polypropylene, 40% Glass Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPH-T40 Homopolymer Polypropylene, 40% Talc Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hypro™ PPC-GF40 Natural Impact Polypropylene, 40% Glass Reinforced Information provided by Entec |
|||
Melt Flow | 10.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
10.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2730B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 10.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU600N ABS Heat Resistant High ImpactInformation provided by Bhansali |
|||
Melt Flow | 10.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
10.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2770 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |