Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.60 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex APEX® 130 Polyvinyl Chloride, Flexible Notes: 80°C Jacket; RoHS CompliantFeatures: Sunlight Resistant (720 hours); Good UV Resistance Uses: Appliance Wire Jacketing; Building Wire Jacketing; Flexible Cord Jacketing; Wire and Cable App.. |
|||
Melt Flow | 1.60 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 1.60 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-97-T0207A-110 Thermoplastic Elastomer Uses: Automotive Applications; Industrial Cable Insulation Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Melt Flow | 1.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Escorene® LD 720.01 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Melt Flow | 1.60 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Escorene® LD 720.62 Specialty Film Resin Escorene Ultra LD 720 resins are high vinyl acetate copolymer specialty film resins designed for applications requiring outstanding heat sealability, along with excellent strength properties and tou.. |
|||
Melt Flow | 1.60 - 23.0 g/10 min | 1.60 - 23.0 g/10 min | Average value: 5.26 g/10 min Grade Count:27 |
Overview of materials for Polystyrene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Flow | 1.60 - 12.0 g/10 min | 1.60 - 12.0 g/10 min | Average value: 5.35 g/10 min Grade Count:13 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |