Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 35.0 g/10 min | 5.00 - 35.0 g/10 min | Average value: 10.3 g/10 min Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Melt Flow | 3.00 - 35.0 g/10 min | 3.00 - 35.0 g/10 min | Average value: 15.6 g/10 min Grade Count:11 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Melt Flow | 0.100 - 35.0 g/10 min | 0.100 - 35.0 g/10 min | Average value: 4.93 g/10 min Grade Count:103 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Melt Flow | 11.0 - 35.0 g/10 min | 11.0 - 35.0 g/10 min | Average value: 20.1 g/10 min Grade Count:7 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Melt Flow | 3.30 - 35.0 g/10 min | 3.30 - 35.0 g/10 min | Average value: 14.6 g/10 min Grade Count:68 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Flow | 3.30 - 35.0 g/10 min | 3.30 - 35.0 g/10 min | Average value: 17.6 g/10 min Grade Count:10 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Melt Flow | 0.400 - 35.0 g/10 min | 0.400 - 35.0 g/10 min | Average value: 8.14 g/10 min Grade Count:9 |
Overview of materials for Polypropylene with Carbon Black Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v.. |