Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 57 g/10 min | 57 g/10 min | ASTM D1238 |
LyondellBasell Alathon® ETP H5057 High Density Polyethylene ApplicationsALATHON H 5057 is a multi-purpose high-flow resin that exhibits enhanced low temperature impact performance, enhanced processability and thermal stability for fast cycling in multi-cavit.. |
|||
Melt Flow | 57 g/10 min @Load 2.16 kg, Temperature 260 °C |
57 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® BF 4215 000000 PBT, 12% Glass Fiber PBT, 12% glass fibers, injection molding, flame retardant |
|||
Melt Flow | 57 g/10 min @Load 2.16 kg, Temperature 250 °C |
57 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1551GN15 PBT, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1551GN15 is a reinforced, flame retardant g.. |
|||
Melt Flow | 57 g/10 min @Load 2.16 kg, Temperature 190 °C |
57 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2715 HDPE Injection Molding Resin
(discontinued **) Features: Excellent low temperature impact strength, good balance of toughness and stiffness, low odor.Applications: Thin walled food containers and lids, frozen and refrigerated containers.Data pro.. |