Physical Properties Metric English Comments
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
NCMT NanoPAC™ HS404 High Performance Polypropylene Nanocomposite
Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Flexirene® MT 40 A Linear Low Density Polyethylene
Flexirene MT 40 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Flexirene MT 40 A is characterized by a good processability and impact r..
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A Condition E; ASTM D1238
Network Polymers NPP 11-5026
Description: Linear Low Density Polyethylene (LLDP)Information provided by Network Polymers Inc.
Melt Flow 50 g/10 min
50 g/10 min
Condition L 230/2.16; ASTM D1238
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an..
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 250 °C
50 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ISO 1133
DuPont Performance Polymers Crastin® CE2055 NC010 PBT  (Unverified Data**)
Crastin® CE2055 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
SABIC M500026 Linear Low Density Polyethylene for Injection Molding
Product Description: M500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excell..
Melt Flow 50 g/10 min

@Load 1.20 kg,
Temperature 300 °C
50 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Melt Volume Rate (ml/10 min); ISO 1133
Chi Mei Wonderloy® PC-175D PC/ABS Alloy  (discontinued **)
Optical Disk
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 2515 MDPE Injection Molding Resin  (discontinued **)
Features: Excellent processability for applications requiring moderate stiffness and improved toughnessExcellent cold temperature impact properties Applications: Ice cream containersHousewares Deep..
Melt Flow 50 - 80 g/10 min
50 - 80 g/10 min
Melt Volume Rate (cm³/10 min)
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether
Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS..
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
M. Holland Company CP850 Polypropylene Impact Copolymer
Impact copolymerFast production cycleHigh flowHigh stiffnessApplications: ContainersHousehold goodsThin-walled parts
Melt Flow 50 g/10 min
50 g/10 min
Intercontinental Polymers HoPBT 545 HoPBT Polymer Type - Clear, Polyester Pellets
Applications: Engineering Resin Information provided by Intercontinental Polymers.
Melt Flow 50 - 80 g/10 min
50 - 80 g/10 min
Melt Volume Rate (cm³/10 min)
Huntsman IROGRAN® A 85 P 4441 TPU-Polyether
Introduction: IROGRAN A 85 P 4441 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 85 P 4441 is part of the HUNTSMAN technical ext..
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Multibase Multi-Flex® A 3540 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodSoftUV Resistance, Go..
Melt Flow 50 g/10 min

@Load 10.0 kg,
Temperature 220 °C
50 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 250 °C
50 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Samyang Tribit® 1500G20 PBT, Reinforced General Purpose
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G20 is a reinforced, general purpose gr..
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Unipetrol PP MONSTEN® MA 350 Polypropylene Homopolymer
Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Wico Plast Wicotal 500 Acetal
ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH
Melt Flow 50 g/10 min
50 g/10 min
ASTM D1238
UBE J5019 Polyethylene
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical prope..
Melt Flow 50 g/10 min
50 g/10 min
ASTM D1238
Total PPC 4944WZ Polypropylene, Impact Copolymer
ATOFINA 4944 polypropylene is a nucleated and controlled rheology impact copolymer. 4944WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. I..
Melt Flow 50 g/10 min

@Temperature 230 °C
50 g/10 min

@Temperature 446 °F
I<sub>2</sub>; ASTM D1238
Formosa Plastics Formolene® 2550A Thin Walled Injection Molding Polypropylene
Medium Impact CopolymerApplications: Housewares, containers and other rigid packaging.Formolene 2550A is a medium impact, high flow, controlled rheology copolymer of polypropylene designed for such ..
Melt Flow 50 g/10 min
50 g/10 min
ASTM D1238
Aclo Accucomp Polyethylene LD0109L Low Density
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 235 °C
50 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Dry)
Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo..
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 275 °C
50 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ISO 1133
BASF Ultradur B 4040 G6 LS High Speed BK15029 30% Glass Filled PBT/PET
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Braskem IG58 HDPE Injection Molding Polyethylene Copolymer
IG58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stiffness, impact strength and out..
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 275 °C
50 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 GF30 Polyamide 6 - Glass Fiber Reinforced
30% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 235 °C
50 g/10 min

@Load 11.0 lb,
Temperature 455 °F
3 min; ASTM D1238
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer
Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized..
Melt Flow 50 g/10 min

@Load 5.00 kg,
Temperature 235 °C
50 g/10 min

@Load 11.0 lb,
Temperature 455 °F
ASTM D1238
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines..
Melt Flow 50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Bapolene® 3295 Polyethylene, Injection Grade
Designed to offer improved cycle times and dimensional stability This product complies with US FDA 21CFR177.1250.Applications: Food containers and closures.Bapolene® and Bapolan® are registered t..
Copyright © lookpolymers.com All Rights Reserved