Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite West Optix® CP - 927 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D-1238 |
Plaskolite Optix® CP - 927 G High Impact Grade Acrylic Resin OPTIX® impact-modified grades offer 7 to 10 times the impact resistance of general purpose polymers while maintaining optical clarity.Information provided by Plaskolite, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM 1238G |
Total Lacqrene® 3351(AS) Impact Polystyrene
(discontinued **) LACQRENE® 3351 is a high heat resistance, high impact polystyrene for injection molding and extrusion/thermoforming. It is recommended for the manufacture of articles which require good dimensiona.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LE-0520-AM LDPE Extrusion Resin
(discontinued **) Features: easy processing, good dispersion.Applications: extrusion coating.Data provided by the manufacturer. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
KKPC Kuhmo GP 125BL Extrusion Molding GPPS Key features: PSP Common Uses: Sheeting, instant noodle cups.GPPS has excellent transparence, colorability, electric property, water-resistance, harmlessness, molding processability, and stability o.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Iran Petrochemical (PCC) HIPS 8350 High Impact Polystyrene HIPS 8350 is a very high impact polystyrene used in the extrusion industry. This grade has an improved environmental stress crack resistance (ESCR) in comparison with standard high impact polystyre.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
LyondellBasell Microthene® G MN72200 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
KKPC Kuhmo GP 150 High Heat Resistant, High Rigidity GPPS Key features: High Heat-resistance, High Strength Common Uses: Vegetable boxes in refrigerators, humidifiers, lighting apparatus, cassette tape cases, parts of optical instruments, PS paper, etc.GPP.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238G |
Hannam Chemical Hanalac 750 ABS, General Purpose FDA Approved. Good combination of impact strength, rigidity, gloss, heat resistance, processability, and thermal stability. May be injection molded. Its broad range of applications include: elect.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 266 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 511 °F |
ASTM D1238 |
SABIC Innovative Plastics Xenoy® X4850 PBT+PC Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional .. |
|||
Melt Flow | 4.5 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.5 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS GN005 Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: GreenInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.5 g/10 min @Load 2.20 kg |
4.5 g/10 min @Load 4.86 lb |
ASTM D1238 |
Sumitomo Chemical ESPOLEX® UT412A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Supreme Petrochem SC 202LV General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability High ClarityProcessing Injection moldingApplications Ball pen barrels, geometrical instruments etc. Suitable for fast cycling products .. |
|||
Melt Flow | 4.5 - 7.5 g/10 min @Temperature 230 °C |
4.5 - 7.5 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 4.5 - 7.5 g/10 min | 4.5 - 7.5 g/10 min | Cond L; ASTM D1238 |
Washington Penn PPUP4G402 Polypropylene, 40% Talc Filled, High Flow Exceptional retention of mechanical properties and appearance upon long term heat aging.Applications: Appliance parts.Data provided by Washington Penn Plastic Co., Inc. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
Westlake EC478AA Low Density Polyethylene WESTLAKE polyethylene EC478 is a low-density resin recommended for use in boardstock coating. This material has an excellent combination of low neck-in, ease of processing and good chill-roll releas.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis CA7230 Low Density Polyethylene CA7230 is a low-density polyethylene for extrusion coating. CA7230 contains no additives. Applications: Extrusion coating of high volume production of boards and papers. Coating of various plasti.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ White LL8425 AP Concentrate Based In LLDPE DescriptionPOLYBATCH® LL8425 AP is an advanced performance white color concentrate containing 45% TiO2 in LLDPE. This product has been specifically engineered to provide improved resistance to phe.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ExxonMobil Method |
ExxonMobil EXACT™ 3024 Plastomer for Cast Film Applications Product Description: Exact 3024 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. It can be used for both monolayer and multilayer coextruded .. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
Buckeye Polymers BP ABS 4332 ABS Low GlossABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing.. |
|||
Melt Flow | 4.5 - 6.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 - 6.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
die 8/2; ISO 1133 |
Addcomp PRIEX® 15005 Maleic Anhydride modified LDPE Functionalised low density polyethylene to be used as compatibiliser for polymer blends or coupling agent for wood flour, natural fibres, or mineral filled polyolefins. Also suitable to reduce pigme.. |
|||
Melt Flow | 4.5 g/10 min | 4.5 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P1-35FM-Y942 35% Glass Fiber/Mineral Reinforced Information provided by Asahi Thermofil |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Exceed™ 4518CB Metallocene Polyethylene Resin Product Description: Exceed 4518 resins are metallocene ethylene-hexene copolymer. Films made from Exceed 4518 have outstanding tensile properties and impact and puncture toughness. These superior p.. |
|||
Melt Flow | 4.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Resirene Resirene® 7600 Super High Impact Polystyrene Features:Medium FlowSuper High ImpactEasy ProcessingHigh ProductivityFDA Rating: 21 CFR 177.1640Applications:InjectionToysCompounds and Master BatchPrintersComputersRemote ControlsInformation provid.. |
|||
Melt Flow | 4.5 g/10 min @Load 2.16 kg |
4.5 g/10 min @Load 4.76 lb |
Condition E; ASTM D1238, ISO 1133 |
DuPont Surlyn® PC2000
(discontinued **) DuPont™ Surlyn® PC2000 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The high MAA c.. |
|||
Melt Flow | 4.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
4.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
cm³/10 min |
Polimeri Europa SINKRAL PD C823 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, exhibiting very high impact resistance, even at low temperatures. Applic.. |