Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PS 160 General Purpose Polystyrene for Foam Extrusion Product Description: General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular .. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 150 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Reliance Industries Repol H033MG Polypropylene REPOL Polypropylene H033MG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Resirene Resirene® 9720 High Impact Polystyrene Features:Medium FlowHigh Thermal ResistantMechanical StrengthFDA Rating: 21 CFR 177.1640Applications:Extrusion/ThermoformingInjectionDisposablesGPPS/HIPS BlendsInformation provided by US distributor.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | ASTM D1238 |
ExxonMobil LL 8401 Rotational Molding Resin
(discontinued **) LL 8401 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for Non-UV applications that require optimum balance of flow processabil.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | ASTM D1238 |
ExxonMobil LL 8401.67 Rotational Molding Resin
(discontinued **) LL 8401 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for Non-UV applications that require optimum balance of flow processabil.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | Exxon Method |
ExxonMobil Escorene® LL-8461 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8400 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8461 is fully formu.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5236 HX HDPE, Impact Grade Medium flow, impact resistant, high stress-crack resistant grade for closures for bottles that contain carbonated liquids. This product contains a slip agent.Data was collected by ISO methods and o.. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
IRPC Polimaxx Polene 330PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Melt Flow | 3.3 g/10 min @Load 10.0 kg, Temperature 260 °C |
3.3 g/10 min @Load 22.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS/PA 1700 B1 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HF-0660I ABS, Unreinforced Material with high flowability and high stiffness that can be used for vacuum cleaner, telephone, TV, VCR, calculator, radio and air-conditionerInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 158 N/L GPPS Styrolution PS 158N/L is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact polystyrene in heat contact applications; for.. |
|||
Melt Flow | 3.3 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.3 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HG-0760 ABS, Unreinforced Used in telephones, vacuum cleaners and electric fan standsInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | 2.16/190; ASTM D1238 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Melt Flow | 3.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
PlastxWorld CEVIAN®-V 450 ABS Heat Resistant ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | 2.16/190; ASTM D1238 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | 2.16/190; ASTM D1238 |
A. Schulman SUPERLINEAR™ XL 0360 Rotational Molding Resin DescriptionSuperlinear XL 0360 is compounded rotational molding resin based on metallocean catalyst technology. This technology allows for high impact and excellent stiffness. It is typically used.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LLP 8460.29 Linear Low Density Polyethylene Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg |
3.3 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 7.7. |
Dow ATTANE™ 4402 Ultra Low Density Polyethylene, Cast Film Grade ATTANE® 4402 copolymer is an ultra low density polyethylene having excellent tear and puncture resistance, and outstanding stretchability. It is designed for industrial/consumer cast film applicati.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg |
3.3 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 7.6. |
Dow DOWLEX™ 2244A Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2244A Polyethylene resin is a cast film polymer having superior optics in packaging applications. This material complies with U.S. FDA Regulation 21 CFR 177.1520 c 3.2 (a) food packaging ap.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow AMPLIFY™ GR 208 Maleic anhydride grafted (MAH) polymer AMPLIFY™ GR 208 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be.. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem ML3601U LLDPE Rotomolding Polyethylene The resin ML3601U is a linear low-density polyethylene, 1-hexene based, with excellent environmental stress cracking resistance and high impact strength. It contains long term UV8 stabilization and .. |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Melt Flow | 3.3 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.3 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Aaron Industries AAROPRENE® AE PC/ABS 7000-2 PC/ABS Engineered Resin Melt flow index may be specified. |
|||
Melt Flow | 3.3 g/10 min @Load 10.0 kg, Temperature 260 °C |
3.3 g/10 min @Load 22.0 lb, Temperature 500 °F |
ASTM D1238 |
Techmer ES Plastiblend® ABS/PA 1700 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Melt Flow | 3.3 g/10 min | 3.3 g/10 min | ASTM D1238 |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |