Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 25.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
25.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Flow | 25.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
25.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Flow | 25.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
25.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East) Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Melt Flow | 25.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
25.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 21 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® MX 1001 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Melt Flow | 25.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
25.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
Calculated from Volume Flow Rate of 21 cm<sup>3</sup>/10min.; ISO 1133 |
Mitsubishi Xantar® MX 1002 Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Melt Flow | 25.2 g/10 min @Load 2.16 kg, Temperature 300 °C |
25.2 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific) LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,.. |