Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D123 |
Niche Polymer PCM18BK PC Information provided by Niche Polymer |
|||
Melt Flow | 18.0 - 24.0 g/10 min @Load 1.106 kg, Temperature 300 °C |
18.0 - 24.0 g/10 min @Load 2.439 lb, Temperature 572 °F |
ASTM D1238 |
Oxford Polymers PC C20-000 Clear PC Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl.. |
|||
Melt Flow | 18.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
18.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1249B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 2104 Thermoplastic Elastomer Features: Nice Silken Feel Uses: Safety ProductsInformation Provided by Teknor Apex |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1625A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1671 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2111S-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2815B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 18.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
18.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2840M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 18.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
18.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® 90-E607B-75NT Ethylene Vinyl Acetate Copolymer Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several.. |
|||
Melt Flow | 18.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
18.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1934A BLK 111 Thermoplastic Elastomer Information Provided by Teknor Apex |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection.. |
|||
Melt Flow | 18.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
18.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2625C Thermoplastic Elastomer Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext.. |
|||
Melt Flow | 18.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
18.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2519F Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 1446A Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |
|||
Melt Flow | 18.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
18.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Elexar® EL 1934A Thermoplastic Elastomer Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti.. |