Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1300 g/10 min | 1300 g/10 min | ASTM D1238, L |
Total PPH 3962 Polypropylene Homopolymer, Ultra-High Melt Flow Rate Pelletized For Melt Blown Fiber Applications High Purity TOTAL Petrochemicals Polypropylene 3962 features extremely high purity for processing into melt blown micro-fibers.Enhanced Productivity. 3962 produces fine denier melt blown micro-fib.. |
|||
Melt Flow | 1300 g/10 min @Load 2.16 kg |
1300 g/10 min @Load 4.76 lb |
|
Dow Primacor® 5990I Ethylene Acrylic Acid (EAA) PRIMACOR® 5990I is an ethylene acrylic acid copolymer (20 wt % comonomer) for specialty hot melt adhesive applications. Its outstanding properties include toughness and adhesion to a wide variety o.. |
|||
Melt Flow | 1300 g/10 min @Load 2.16 kg, Temperature 230 °C |
1300 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem H 155 Fiber Extrusion Polypropylene Homopolymer Meltblown nonwoven applications for hygienic, medical and hospital disposable devices; Filters and oil adsorbents.Information provided by Braskem. |