Polymer Property : Melt Flow = 110 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 110 g/10 min

@Load 2.16 kg,
Temperature 180 °C
110 g/10 min

@Load 4.76 lb,
Temperature 356 °F
Hybrid Plastics Polyamide POSS® Flow Masterbatch
POSS® Flow masterbatches show success in reducing the melt viscosity of a variety of injection molded and extruded resins. Hybrid Plastics now introduces such a solution for polyamide polymers. P..
Melt Flow 110 g/10 min
110 g/10 min
ASTM D1238
Flint Hills P9H9Z-018 Polypropylene
Specialty polypropylene, UL certified, and FDA compliant.Applications: Extrusion coating.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Melt Flow 110 g/10 min

@Load 10.0 kg,
Temperature 400 °C
110 g/10 min

@Load 22.0 lb,
Temperature 752 °F
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera..
Melt Flow 110 g/10 min

@Load 2.16 kg,
Temperature 230 °C
110 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Borealis RJ900MO Polypropylene Random Copolymer
RJ900MO is a polypropylene random copolymer with high melt flow and good transparency. Products originating from this grade have excellent transparency and gloss, and good balance of stiffness and ..
Melt Flow 110 g/10 min

@Load 2.16 kg,
Temperature 230 °C
110 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Total Lumicene® MR110MC2 Metallocene Random Copolymer Polypropylene, Injection Molding
Lumicene® MR110MC2 is a metallocene random copolymer with a melt flow index of 110 g/10 min for injection molding. This Lumicene® MR110MC2 high fluidity differs from standard random copolymers by ..
Melt Flow 110 g/10 min

@Load 5.00 kg,
Temperature 260 °C
110 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Goodfellow TPX® DX350 Coating/Extrusion Grade Polymethylpentene
This grade is highly recommended for paper coating or for fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release characteristics a..
Melt Flow 110 g/10 min

@Load 2.16 kg,
Temperature 230 °C
110 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Braskem TI2900C High Crystallinity Copolymer Polypropylene
Description: Highly Crystalline Homopolymer Phase, Very High Molecular Weight EPR Phase, Very High Flexural Modulus, Reduced Emissions, Reduced Gels.Applications: Suggested uses include compounding...
Melt Flow 110 g/10 min

@Load 5.00 kg,
Temperature 275 °C
110 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Transparent up to maximum 2.5 mm.Tarnamid® has the following main properties..
Melt Flow 110 g/10 min

@Load 10.0 kg,
Temperature 275 °C
110 g/10 min

@Load 22.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultradur B 4040 G10 LS High Speed BK15029 50% Glass Filled PBT/PET
Melt Flow 110 g/10 min

@Load 5.00 kg,
Temperature 266 °C
110 g/10 min

@Load 11.0 lb,
Temperature 511 °F
ASTM D1238
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.
Copyright © lookpolymers.com All Rights Reserved