Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 11.9 g/10 min @Load 5.00 kg, Temperature 280 °C |
11.9 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Melt Flow | 11.9 g/10 min @Load 5.00 kg, Temperature 280 °C |
11.9 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Melt Flow | 11.9 g/10 min @Load 5.00 kg, Temperature 280 °C |
11.9 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Europe-Africa-Middle East) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Melt Flow | 11.9 g/10 min @Load 2.16 kg, Temperature 235 °C |
11.9 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BECN P20 TL Nylon 11 (Dry) ISO data provided by the manufacturer, Arkema. |
|||
Melt Flow | 11.9 g/10 min @Load 2.16 kg, Temperature 235 °C |
11.9 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BECN P20 TL Nylon 11 (Conditioned) ISO data provided by the manufacturer, Arkema. |