Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.10 - 122 g/10 min | 1.10 - 122 g/10 min | Average value: 32.1 g/10 min Grade Count:26 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Melt Flow | 1.10 - 11.0 g/10 min | 1.10 - 11.0 g/10 min | Average value: 5.88 g/10 min Grade Count:9 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Melt Flow | 1.10 - 50.0 g/10 min | 1.10 - 50.0 g/10 min | Average value: 17.4 g/10 min Grade Count:3 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Melt Flow | 1.10 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.10 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4764A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 1.10 - 22.7 g/10 min | 1.10 - 22.7 g/10 min | Average value: 3.63 g/10 min Grade Count:24 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Melt Flow | 1.10 - 20.0 g/10 min | 1.10 - 20.0 g/10 min | Average value: 5.68 g/10 min Grade Count:16 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |
|||
Melt Flow | 1.10 - 26.0 g/10 min | 1.10 - 26.0 g/10 min | Average value: 4.90 g/10 min Grade Count:13 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Flow | 1.10 - 9.80 g/10 min | 1.10 - 9.80 g/10 min | Average value: 4.93 g/10 min Grade Count:4 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |