Physical Properties Metric English Comments
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 29MB080 OPP Film
Product Description: A biaxially oriented polypropylene film metallizable on one side, with a heat sealable surface on the other side. Designed to be used after metallization as a single web in HFFS..
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MB400 OPP Film
Product Description: A heat sealable coextruded biaxially oriented polypropylene film that can be used on a wide range of packaging machines. 30MB400 can be either used as mono material or in lamina..
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MB666 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MB668 OPP Film
Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side very low temperature seal (VLTS) coating. VLTS coating provides excellent performances on high s..
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MBR666 OPP Film
Product Description: Bicor 30MBR is a biaxially oriented transparent polypropylene film coated with humidity resistant acrylic on both sides. This film is designed to wrap products with a high moist..
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 35MD447 OPP Film
Product Description: A coextruded super white opaque, modified high density, biaxially oriented polypropylene film, heat sealable on both sides. This opaque and extremely stiff film is ideal for use..
Water Vapor Transmission 1.01 g/m²/day

@Temperature 23.0 °C
0.0650 g/100 in²/day

@Temperature 73.4 °F
85% RH; ExxonMobil Method
ExxonMobil Bicor™ 30MBT666 OPP Film