Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips SUPER-STA NLGI No. 1 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips SUPER-STA NLGI No. 2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | |
ConocoPhillips Syncon® 75W-90 HP Synthetic Gear Oil Description: Conoco Syncon HP Synthetic Gear Oil is recommended for conventional and limited-slip differentials, as well as some manual transmissions commonly found in passenger cars, race cars, tru.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips Tacna® 2000 NLGI No. 2 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | |
ChevronTexaco ISO 220 Marine Oil E FeaturesChevron Marine Oils E are formulated using a blend of high grade, medium viscosity index base oils and carefully balanced additive package to meet the crankcase need of marine steam engines... |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | ASTM D-2161 |
ConocoPhillips ANDEROL® PQ AA 90 White Mineral Food Grade Gear Oil, ISO Grade 220, SAE Gear Oil Grade 90 Description: ANDEROL PQ AA Series Gear Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Gear.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips EP Conolith® Grease NLGI NO. 0 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips EP Conolith® Grease NLGI NO. 00 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips EP Conolith® Grease NLGI NO. 000 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips EP Conolith® Grease NLGI NO. 1 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips EP Conolith® Grease NLGI NO. 2 Description: Conoco EP Conolith Grease is a high-quality, multipurpose, extreme pressure lithium grease recommended for heavy-duty, heavily loaded antifriction and plain bearings. It is ideal for th.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | |
ConocoPhillips Hydroclear® 20W-50 High Performance Motor Oil SAE 20W-50 Description: Conoco Hydroclear High Performance Motor Oil SAE 20W-50, formulated with premium base stocks, lubricates gasoline engines that operate under severe driving conditions. It is particularl.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips SUPER-STA M NLGI No.0 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips SUPER-STA M NLGI No.2 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips Tacna® 2000 NLGI No. 1 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Saybolt Viscosity at 210°F | 86 SUS | 86 SUS | Base Oil Property |
ConocoPhillips SUPER-STA M NLGI No.1 Description: Conoco Super-STA and Super-STA M Greases are premium-quality, extreme-pressure (EP), multipurpose lithium greases recommended for lubrication of wheel bearings, chassis, ball joints, C... |