Physical Properties | Metric | English | Comments |
---|---|---|---|
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco 100 Honor Ashless AW Texaco Honor Ashless AW are circulating oils formulated from high quality base stocks and a carefully balanced, zinc-free additive package. These proved excellent protection against wear for long be.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco Aries® 100 Texaco Aries lubricants deliver value through:Long equipment life — Extreme pressure performance withstands heavy shock loads typical of rock drill service, protecting the equipment against rapid w.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco Canopus® 100 Texaco Canopus oils deliver value through:High resistance to forming emulsions due to excellent water separating characteristics.Long lubricant life provided by outstanding stability.Good lubricant .. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco Gear Compounds EP, ISO 100 FeaturesChevron Gear Compounds EP are multipurpose gear lubricants.They provide good thermal stability, extreme pressure
protection, antiwear and demulsibility, oxidation, rust, corrosion control an.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco ISO 100 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco ISO 100 Machine Oil AW FeaturesChevron Machine Oils AW are premium quality lubricants.They provide excellent antiwear protection, oxidation and corrosion inhibition, and foam and aeration suppression.They are excellent mu.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco ISO 100 Red Chain Bar Oil FeaturesChevron Red Chain Bar Oils are very tacky, tough, lubricants made from special high viscosity base oils having the desired flow and pumpability properties to assure adequate lubrication over.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco ISO 100 Utility Oil HVI FeaturesChevron Utility Oil HVI is a high quality, high viscosity index uncompounded oil with excellent water separating characteristics.Chevron Utility Oil HVI possesses good natural thermal and ox.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco Meropa® 100 Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco Rando® HD 100 Texaco Rando HD oils deliver value through:Longer equipment life — Special antiwear additive package reduces wear by protecting surfaces when load causes breakdown of the lubricant film.Reduced dow.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | ASTM D445 |
ChevronTexaco Regal® 100 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco Vistac® ISO 100 Rock Drill Oil FeaturesChevron Rock Drill Oils Vistac are designed to give maximum protection to percussion rock drills.They are formulated from highly refined, high viscosity index, paraffinic base stocks and add.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco Chain, Bar, and Sprocket Lubricant Texaco Chain, Bar and Sprocket Lubricant delivers value through:Reduced wear — Minimize wear for the chain, bar, and sprocket.Tackiness — The increased tackiness additive keeps the oil on the chai.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ChevronTexaco GST® ISO 100 Oil FeaturesChevron GST Oils are designed to meet the critical demands of:gas, steam, and hydroelectric turbine bearing lubricationreduction gear lubrication in marine operationsThey are an excellent re.. |
|||
Saybolt Viscosity at 100°F | 495 SUS | 495 SUS | |
ConocoPhillips Hydroclear Diamond Class® 100 Turbine Oil Description: Conoco Hydroclear Diamond Class Turbine Oil is an extended service life rust- and oxidation-inhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Di.. |