Physical Properties | Metric | English | Comments |
---|---|---|---|
Oxidative Induction Time (OIT) | >= 50 min | >= 50 min | ASTM D3895 |
Reliance Industries Relene D16501 Polyethylene Relene D16501 is a UV stabilized High Density Polyethylene compound with broad molecular weight distributions, suitable for producing cable duct for optic fiber and other general purpose cables. Th.. |
|||
Oxidative Induction Time (OIT) | 50 min | 50 min | At 200°C, Al-pan; ASTM D3895 |
Borealis Borcell™ HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables Borcell HE1344 is a high-molecular weight, high-density polyethylene (HDPE) insulation compound containing an industry approved non plate-out chemical blowing agent. It contains the required levels.. |
|||
Oxidative Induction Time (OIT) | >= 50 min @Temperature 200 °C |
>= 50 min @Temperature 392 °F |
IEC 60811-4-2/B |
Borealis Borcell™ HE1346 High Density Polyethylene Borcell™ HE1346 is a fully formulated compound for chemical foamed telesingles. Borcell™ HE1346 is a high-density polyethylene compound containing chemical blowing agent.
Applications Borcell™ HE.. |
|||
Oxidative Induction Time (OIT) | 50 min @Temperature 200 °C |
50 min @Temperature 392 °F |
IEC 60811-4-2/B |
Borealis Borcell™ ME1244 Medium Density Polyethylene Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 i.. |
|||
Oxidative Induction Time (OIT) | >= 50 min @Temperature 210 °C |
>= 50 min @Temperature 410 °F |
EN 728 |
Borealis BorPEX™ HE1878E-C2 High Molecular Weight Polyethylene, Crosslinkable BorPEX™ HE1878E-C2 is a high molecular weight, high density polyethylene specially designed for production of cross linked pipes (PE-X). Applications: BorPEX™ HE1878E-C2 is recommended for the pr.. |
|||
Oxidative Induction Time (OIT) | 50 min @Temperature 200 °C |
50 min @Temperature 392 °F |
IEC 60811-4-2/B |
Borealis HE3366 High Density Polyethylene HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer sk.. |
|||
Oxidative Induction Time (OIT) | 50 min @Temperature 200 °C |
50 min @Temperature 392 °F |
IEC 60811-4-2/B |
Borealis ME6032 Polypropylene ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S.. |
|||
Oxidative Induction Time (OIT) | >= 50 min @Temperature 220 °C |
>= 50 min @Temperature 428 °F |
ASTM-D3895 |
Braskem PCD 0140 HECO Polypropylene Heterophasic Copolymer PCD 0140 is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140 is highly protected against thermal aging and.. |
|||
Oxidative Induction Time (OIT) | >= 50 min @Temperature 220 °C |
>= 50 min @Temperature 428 °F |
ASTM-D3895 |
Braskem PCD 0140BR HECO Polypropylene Heterophasic Copolymer PCD 0140BR is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140BR is highly protected against thermal aging.. |