Polymer Property : Oxidative Induction Time (OIT) = 50 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Oxidative Induction Time (OIT) >= 50 min
>= 50 min
ASTM D3895
Reliance Industries Relene D16501 Polyethylene
Relene D16501 is a UV stabilized High Density Polyethylene compound with broad molecular weight distributions, suitable for producing cable duct for optic fiber and other general purpose cables. Th..
Oxidative Induction Time (OIT) 50 min
50 min
At 200°C, Al-pan; ASTM D3895
Borealis Borcell™ HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables
Borcell HE1344 is a high-molecular weight, high-density polyethylene (HDPE) insulation compound containing an industry approved non plate-out chemical blowing agent. It contains the required levels..
Oxidative Induction Time (OIT) >= 50 min

@Temperature 200 °C
>= 50 min

@Temperature 392 °F
IEC 60811-4-2/B
Borealis Borcell™ HE1346 High Density Polyethylene
Borcell™ HE1346 is a fully formulated compound for chemical foamed telesingles. Borcell™ HE1346 is a high-density polyethylene compound containing chemical blowing agent. Applications Borcell™ HE..
Oxidative Induction Time (OIT) 50 min

@Temperature 200 °C
50 min

@Temperature 392 °F
IEC 60811-4-2/B
Borealis Borcell™ ME1244 Medium Density Polyethylene
Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 i..
Oxidative Induction Time (OIT) >= 50 min

@Temperature 210 °C
>= 50 min

@Temperature 410 °F
EN 728
Borealis BorPEX™ HE1878E-C2 High Molecular Weight Polyethylene, Crosslinkable
BorPEX™ HE1878E-C2 is a high molecular weight, high density polyethylene specially designed for production of cross linked pipes (PE-X). Applications: BorPEX™ HE1878E-C2 is recommended for the pr..
Oxidative Induction Time (OIT) 50 min

@Temperature 200 °C
50 min

@Temperature 392 °F
IEC 60811-4-2/B
Borealis HE3366 High Density Polyethylene
HE3366 is a HDPE compound for solid insulation of telephone singles with high extrusion speed. HE3366 is designed as insulation for petroleum filled telephone cables. It is also suitable as outer sk..
Oxidative Induction Time (OIT) 50 min

@Temperature 200 °C
50 min

@Temperature 392 °F
IEC 60811-4-2/B
Borealis ME6032 Polypropylene
ME6032 is a MDPE compound for solid insulation of telephone singles and data cables at high line speed. It contains a metal deactivator. Applications: Dry core and petroleum jelly filled cables. S..
Oxidative Induction Time (OIT) >= 50 min

@Temperature 220 °C
>= 50 min

@Temperature 428 °F
ASTM-D3895
Braskem PCD 0140 HECO Polypropylene Heterophasic Copolymer
PCD 0140 is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140 is highly protected against thermal aging and..
Oxidative Induction Time (OIT) >= 50 min

@Temperature 220 °C
>= 50 min

@Temperature 428 °F
ASTM-D3895
Braskem PCD 0140BR HECO Polypropylene Heterophasic Copolymer
PCD 0140BR is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140BR is highly protected against thermal aging..