Physical Properties | Metric | English | Comments |
---|---|---|---|
Pore Size | 0.00700 microns | 0.000276 mil | Average Diameter |
NanoScale NanoActive® Cerium Oxide NanoActive CeO2 is produced using proprietary processes to obtain high specific surface area, aggregated dry powder that can be dispersed in various carrier fluids to significantly reduce the partic.. |