Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.850 - 1.00 g/cc | 0.0307 - 0.0361 lb/in³ | ISO 60 |
Raschig Group 3505 Epoxy Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed.. |
|||
Apparent Bulk Density | 0.850 - 1.00 g/cc | 0.0307 - 0.0361 lb/in³ | ISO 60 |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Apparent Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | ASTM D4894 |
3M Dyneon™ 1620 PTFE Powder
(discontinued **) Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a.. |
|||
Apparent Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | 80 pellets/g, Limit; M2E-72-015 |
Indorama Ventures Mexico Polyclear™ Refresh 1101 PET Resin Description: La resina Polyclear® Refresh PET 1101 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen.. |
|||
Apparent Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | Limit; M2E-72-015 |
Indorama Ventures Mexico Polyclear™ Splash 3301 PET Resin Description: La resina Polyclear® Splash PET 3301 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.74 dl/g. La resina Polyclear® Splash PET 3301 ha sido .. |
|||
Apparent Bulk Density | 0.850 - 0.950 g/cc | 0.0307 - 0.0343 lb/in³ | Limit; M2E-72-015 |
Indorama Ventures Mexico Polyclear™ T-94 PET Resin Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de.. |
|||
Apparent Bulk Density | 0.850 g/cc | 0.0307 lb/in³ | TRM-37 |
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |