Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.760 g/cc | 0.0275 lb/in³ | DIN 53 466 |
3M Dyneon™ TF 4220 PTFE 2% Cond. Pigm. Filled
(discontinued **) Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon. |
|||
Apparent Bulk Density | 0.760 g/cc | 0.0275 lb/in³ | |
Sumitomo Bakelite North America 51-01 CAFR-P Mineral Filled Diallyl Phthalate Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ.. |
|||
Apparent Bulk Density | 0.760 g/cc | 0.0275 lb/in³ | |
Cosmic Plastics E4920 Mineral Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Apparent Bulk Density | 0.760 g/cc | 0.0275 lb/in³ | DIN 53 466 |
3M Dyneon™ TFM™ 4220 Modified PTFE, 2% Cond. Pigm. Filled
(discontinued **) Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon. |