Physical Properties Metric English Comments
Apparent Bulk Density 0.00900 - 0.650 g/cc
0.000325 - 0.0235 lb/in³
Average value: 0.0682 g/cc Grade Count:21
Overview of materials for Expanded Polystyrene (EPS)
This property data is a summary of similar materials in the MatWeb database for the category "Expanded Polystyrene (EPS)". Each property range of values reported is minimum and maximum values of app..
Apparent Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
Average value: 0.576 g/cc Grade Count:17
Overview of materials for PVC, Rigid Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M..
Apparent Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
MSZ ISO 60:1994
BorsodChem ONGROSTYR F-I Expandable Polystyrene (EPS)
ONGROSTYR F-I is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e...
Apparent Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
MSZ ISO 60:1994
BorsodChem ONGROSTYR F-IV Expandable Polystyrene (EPS)
ONGROSTYR F-IV is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e..
Apparent Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
MSZ ISO 60:1994
BorsodChem ONGROSTYR F-II Expandable Polystyrene (EPS)
ONGROSTYR F-II is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i.e..
Apparent Bulk Density 0.550 - 0.650 g/cc
0.0199 - 0.0235 lb/in³
MSZ ISO 60:1994
BorsodChem ONGROSTYR F-III Expandable Polystyrene (EPS)
ONGROSTYR F-III is an expandable, flame-retardant styrene homopolymer, produced by suspension polymerization. The product meets the requirements of DIN 4102 and of B1 class of building materials, i...