Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 3.13 g/cc | 0.113 lb/in³ | |
Poco Graphite SUPERSiC® Basic Silicon Carbide The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for.. |