Physical Properties Metric English Comments
Apparent Bulk Density 0.850 - 1.00 g/cc
0.0307 - 0.0361 lb/in³
ISO 60
Raschig Group 3505 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. This product meets the allowed..
Apparent Bulk Density 0.850 - 1.00 g/cc
0.0307 - 0.0361 lb/in³
ISO 60
Raschig Group 3535 Epoxy
Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack..
Apparent Bulk Density 0.850 g/cc
0.0307 lb/in³
ASTM D4894
3M Dyneon™ 1620 PTFE Powder  (discontinued **)
Type II, gr. 3 PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a..
Apparent Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
80 pellets/g, Limit; M2E-72-015
Indorama Ventures Mexico Polyclearâ„¢ Refresh 1101 PET Resin
Description: La resina Polyclear® Refresh PET 1101 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen..
Apparent Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
Limit; M2E-72-015
Indorama Ventures Mexico Polyclearâ„¢ Splash 3301 PET Resin
Description: La resina Polyclear® Splash PET 3301 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.74 dl/g. La resina Polyclear® Splash PET 3301 ha sido ..
Apparent Bulk Density 0.850 - 0.950 g/cc
0.0307 - 0.0343 lb/in³
Limit; M2E-72-015
Indorama Ventures Mexico Polyclearâ„¢ T-94 PET Resin
Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de..
Apparent Bulk Density 0.850 g/cc
0.0307 lb/in³
TRM-37
Tipco Tipcolite® THD 411 Phenolic Compound, Mica, Asbestos & Cellulose, Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Mica, Asbestos & CelluloseApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr..