Polymer Property : Apparent Bulk Density = 0.425 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.425 g/cc
0.0154 lb/in³
ISO 1068
Arkema Group ORGASOL® 1002 D Nat 1 Polyamide 6
Information provided by Arkema Group
Apparent Bulk Density 0.425 g/cc
0.0154 lb/in³
ISO 1068
Arkema Group ORGASOL® 1002 ES 4 Nat 1 Polyamide 6
Information provided by Arkema Group
Apparent Bulk Density 0.425 g/cc
0.0154 lb/in³
ISO 1068
Arkema Group ORGASOL® 2002 ES 4 Nat 3 Polyamide 12
Information provided by Arkema Group
Apparent Bulk Density 0.425 g/cc
0.0154 lb/in³
ISO 1068
Arkema Group ORGASOL® 2002 ES 6 Nat 3 Polyamide 12
Information provided by Arkema Group
Apparent Bulk Density 0.425 g/cc
0.0154 lb/in³
ISO 1068
Arkema Group ORGASOL® 2002 ES 5 Nat 3 Polyamide 12
Information provided by Arkema Group
Apparent Bulk Density 0.425 - 0.800 g/cc
0.0154 - 0.0289 lb/in³
Average value: 0.650 g/cc Grade Count:12
Overview of materials for Nylon 6, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri..