Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 4.0 - 8.0 cP | 4.0 - 8.0 cP | 20% aq. Sol.; L170 |
Solvay GLOKILL® PQ60 Surfactant Description: Algicide and biocide for swimming poolIdentification: POLYQUARTERNARY AMMONIUM CHLORIDE, AQUEOUS SOLUTIONCAS: 25988 – 97 – 0Available in: EuropeFunction: Algaecide for use in .. |
|||
Viscosity | 4.0 - 8.0 cP | 4.0 - 8.0 cP | |
Daikin NEOFLON ND-2 FEP Dispersion, Milky White NEOFLON FEP dispersions are fine-powder suspension. Two types are available: water based and organic solvent based. Since FEP has good flowability when melted, a continuous, pinhole-free film can .. |
|||
Viscosity | 3.0 - 8.0 cP | 3.0 - 8.0 cP | U-Tube IC-C45 |
3M Scotch-Weld™ MG05 LO Medical Grade Instant Adhesive 3M™ Scotch-Weld™ Medical Grade Instant Adhesive are intended for use on a wide variety of materials used in the construction of disposable medical assemblies. They will quickly bond metals, plasti.. |