Physical Properties Metric English Comments
Viscosity 2300 - 3800 cP
2300 - 3800 cP
ND Industries Toughened Ethyl SuperGlue 310
Black flexible Cyanoacrylate for metal, rubber, and plastic
Viscosity 2800 - 3800 cP

@Temperature 23.0 °C
2800 - 3800 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® H20E-175 Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-175 is a two component epoxy designed for semiconductor die-attach. It is a higher Tg version of EPO-TEK® H20E. It was designed to be used in semiconductor / J..