Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2300 - 2800 cP | 2300 - 2800 cP | |
ND Industries SuperGlue Ethyl 322 High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III |
|||
Viscosity | 1800 - 2800 cP @Temperature 23.0 °C |
1800 - 2800 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping Product Description: EPO-TEK® H20S is a modified version of EPO-TEK® H20E, designed primarily for die stamping and dispensing techniques for chip bonding. EPO-TEK®H20S is a highly reliable, two .. |
|||
Viscosity | 1800 - 2800 cP @Temperature 23.0 °C |
1800 - 2800 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® H20E-LV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-LV is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a .. |