Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1600 - 2300 cP @Temperature 180 - 180 °C |
1600 - 2300 cP @Temperature 356 - 356 °F |
Average value: 2080 cP Grade Count:4 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Viscosity | 800 - 2300 cP | 800 - 2300 cP | |
Huntsman HZ 815 X-70 US Aromatic Amine Approx. H+ equivalent weight 150. Mix Ratio with GY 6010 is 81.Comments/Applications: Solution of HY 815, 70% solids in xylene. Trade sale paint enamels. Industrial maintenance, FDA. Flexible m.. |
|||
Viscosity | 1400 - 2300 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1400 - 2300 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2070209P6 White Dielectric Paste This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 2000 - 2300 cP @Temperature 23.0 °C |
2000 - 2300 cP @Temperature 73.4 °F |
|
Master Bond EP42LV Low Viscosity Chemically Resistant Two Component Epoxy System Master Bond Polymer System EP42LV is a low viscosity room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring outstanding chemical
resistance. While EP.. |
|||
Viscosity | 600 - 2300 cP | 600 - 2300 cP | Milled Cement; Zeon Test #327 |
Zeon Chemicals Nipol® 1000x88 Nitrile Elastomer Nipol 1000X88 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient antioxidant is added during manufacture for normal storage conditions.Excellent in adhesives whe.. |