Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 28000 - 130000 cP @Temperature 204 - 204 °C |
28000 - 130000 cP @Temperature 399 - 399 °F |
Average value: 83800 cP Grade Count:4 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Viscosity | 1000 - 130000 cP @Temperature 40.0 - 105 °C |
1000 - 130000 cP @Temperature 104 - 221 °F |
Average value: 19400 cP Grade Count:7 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Viscosity | 115000 - 130000 cP | 115000 - 130000 cP | A |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Viscosity | 80000 - 130000 cP | 80000 - 130000 cP | |
Master Bond EP17HT-3 One component, snap-curing epoxy system Product Description: Master Bond Polymer System EP17HT-3 is a one part epoxy that fully cures in 2-3 minutes at 250-300°F. It is capable of service up to +400°F with excellent strength retention p.. |
|||
Viscosity | 90000 - 130000 cP | 90000 - 130000 cP | |
Master Bond EP36AN One Part, Toughened, B-Stage Epoxy Description: Master Bond EP36AN is a unique one component, high performance epoxy for bonding, encapsulation, potting and coating featuring thermal conductivity, electrical insulation and high tempe.. |
|||
Viscosity | 60000 - 130000 cP | 60000 - 130000 cP | Accelerator |
3M Scotch-Weld™ DP420 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |