Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.400 - 1.10e+6 cP | 0.400 - 1.10e+6 cP | Average value: 17700 cP Grade Count:373 |
Overview of materials for Cyanoacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Viscosity | 1.00 - 1.10e+6 cP | 1.00 - 1.10e+6 cP | Average value: 25300 cP Grade Count:229 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | 700000 - 1.10e+6 cP @Shear Rate 100 1/s, Temperature 232 °C |
700000 - 1.10e+6 cP @Shear Rate 100 1/s, Temperature 450 °F |
Melt Viscosity; ASTM D3835 |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Viscosity | 500000 - 1.10e+6 cP | 500000 - 1.10e+6 cP | at 2.5 RPM |
Loctite® Output™ 383 Acrylic Adhesive Acrylic Bonding Adhesives and Thermally Conductive BondersLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impa.. |