Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 90 - 120 cP | 90 - 120 cP | |
ND Industries 301 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Viscosity | 90 - 120 cP | 90 - 120 cP | |
ND Industries SuperGlue Ethyl 314 General DescriptionA medium viscosity ethyl-based cyanoacrylate particularly suitable for rubbers and plastics. It is fast acting and may be fillet cured using ND Excel Accelerators.rubber O-rings,.. |
|||
Viscosity | 90 - 120 cP | 90 - 120 cP | |
ND Industries SuperGlue Methyl 330 Low-Medium Viscosity - General purpose metal surfaceMeets military spec Mil-A-46050C Type I Class II |
|||
Viscosity | 90 - 110 cP | 90 - 110 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130 - MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moistur.. |
|||
Viscosity | 90 - 110 cP | 90 - 110 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 130 (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 90 - 110 cP | 90 - 110 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 130 CLEAR FLEXIBLE (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 440 - GEL BLACK TOUGHENED advanced thixotropic formula is designed to polymerize instantly by absorbing surface .. |
|||
Viscosity | 90 - 110 cP | 90 - 110 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 130 LOW ODOR/LOW BLOOM (100 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130 LOW ODER advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's p.. |
|||
Viscosity | 90 - 110 cP | 90 - 110 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 130PR PLASTIC & RUBBER (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130PR PLASTIC & RUBBER’S advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Viscosity | 90 - 110 cP | 90 - 110 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 130SI Surface Insensitive (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Viscosity | 90 - 500 cP @Temperature 25.0 °C |
90 - 500 cP @Temperature 77.0 °F |
|
Northstar Polymers MNB-013 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 90 cP | 90 cP | |
Resin Technology Group 60 Low Odor, Low Bloom Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 60 Low Odor, Low Bloom Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 90 - 110 cP @Temperature 25.0 °C |
90 - 110 cP @Temperature 77.0 °F |
Uncured |
Permabond 802 Cyanoacrylate, High Temperature PERMABOND® 802 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Viscosity | 90 - 110 cP @Temperature 25.0 °C |
90 - 110 cP @Temperature 77.0 °F |
Uncured |
Permabond 820 Cyanoacrylate, High Temperature PERMABOND® 820 is a low viscosity modified ethyl cyanoacrylate suitable for applications where high temperature resistance is required. This material is fast setting and has good adhesion to rubber.. |
|||
Viscosity | 90 cP | 90 cP | Viscosity of Solution; 5% Styrene |
KKPC KOSYN KBR 710L Polybutadiene Rubber (Low cis BR) Polybutadiene Rubber (Low cis BR)Characteristics: Low cis BR is different in cis content according to the production process and the catalyst. KKPC's low cis LBR has 35% cis content. LBR has hi.. |
|||
Viscosity | 90 cP | 90 cP | |
Lord Adhesives 6900 Medium Viscosity, Low Odor, Low Bloom Butyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Viscosity | 90 cP | 90 cP | |
Lord Adhesives 7000 Medium Setting, Medium Viscosity, Moisture Resistant Methyl Cyanoacrylate Adhesive Lord Cyanoacrylate AdhesivesLord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metal.. |
|||
Viscosity | 90 - 100 cP | 90 - 100 cP | |
Master Bond Mastersil 718 Adhesion Enhancement Silicone Primer MasterSil Primer 718 is a specially formulated silicone primer for use with MasterSil RTV silicone elastomers and sealants to promote adhesion to various difficult-to-bond substrates such
as acrylic.. |
|||
Viscosity | 90 cP | 90 cP | Nominal |
Dymax Light Weld® 401 High Clarity Glass Bonding Adhesive Glass Bonding in SecondsDescriptionDymax Light Weld® 400 Series adhesives form high-clarity, invisible bonds between glass and other substrates in seconds. In addition to many structural glass bond.. |
|||
Viscosity | 90 cP | 90 cP | A Component; ASTM D1824 |
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e.. |
|||
Viscosity | 90 cP | 90 cP | |
3M Scotch-Weld™ MG90-77 UV Medical Grade Light Cure Adhesive 3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing .. |
|||
Viscosity | 90 - 110 cP @Temperature 25.0 °C |
90 - 110 cP @Temperature 77.0 °F |
Uncured |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |