Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 650 - 750 cP | 650 - 750 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 155-HT (700 cp HIGH TEMPERATURE) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 190-HT advanced formula is designed to polymerize instantly by absorbing surface moisture and is recommended for.. |
|||
Viscosity | 650 - 1950 cP | 650 - 1950 cP | |
Lord Adhesives 312 General Purpose, Low Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Viscosity | 650 cP | 650 cP | |
Solvay ANTAROX® L 64 Surfactant Description: EO.PO block polymer with high cloud point. Multipurpose emulsifier. Dispersing agent. Suggested for emulsifiable concentrates with polar solvents.Chemical Name: EO/PO BLOCK COPOLYMERCAS.. |
|||
Viscosity | 650 - 1200 cP @Temperature 125 °C |
650 - 1200 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® E-10 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Epolene® E-Type Polymers are easily emulsifiable, available in PE and PP based materials, and approved by the FDA for food contact. They have a wide ring & ball softening point range, oil and water.. |
|||
Viscosity | 650 cP @Temperature 25.0 °C |
650 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 832-5 Flexible Epoxy TRA-BOND 832-5 is a flexible two component epoxy which is intended for bonding materials with mis-matched coefficients of expansion. It exhibits flexibility associated with polyurethanes but does no.. |
|||
Viscosity | 650 cP | 650 cP | |
Von Roll Isola IMI Varnish 74001 Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 24°C. Average solids: 92.5%. Usage Notes: Clear epoxy insulating varnish which penetrates and saturates extremely well, giving outstanding moisture .. |
|||
Viscosity | 650 cP @Temperature 25.0 °C |
650 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond F109 Fiber Optic Epoxy Adhesive TRA-BOND F109 is specially designed to be used in fiber optic connectors where connections must be made in high humidity environments. This two part, low viscosity epoxy remains at a constant viscos.. |
|||
Viscosity | 650 cP @Temperature 180 °C |
650 cP @Temperature 356 °F |
Melt; ETM 22-31 |
ExxonMobil ESCOREZ™ 5615 Petroleum Hydrocarbon Resin Very light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefins. A.. |
|||
Viscosity | 650 cP | 650 cP | |
Dymax 957 Potting and Encapsulation Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 957 Potting and Encapsulation AdhesiveDesigned to adhere to a wide variety of materials, high strength. Cure Type: U.. |
|||
Viscosity | 650 - 750 cP @Temperature 30.0 °C |
650 - 750 cP @Temperature 86.0 °F |
|
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Viscosity | 650 cP | 650 cP | |
BASF Lupranate® 5090 Isocyanate Description: Lupranate® 5090 Isocyanate is a liquid prepolymer of pure, diphenylmethane diisocyanate (MDI). The Lupranate 5090 Isocyanate has been formulated for improved low-temperature stability .. |
|||
Viscosity | 650 cP | 650 cP | A Side |
ACC EP AJS EPI Engineered Polymers Aliphatic Joint Sealant EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint seala.. |
|||
Viscosity | 650 cP | 650 cP | B Side |
ACC EP LCP EPI Engineered Polymers Aromatic Polyurea EP LCP Aromatic Polyurea, “Powered by Reactamine® Technology” is a two component 100% solid Polyurea (silicone optional) with superior performance in industrial applications. EP LCP displays extr.. |
|||
Viscosity | 650 cP | 650 cP | uncatalyzed, Deep Section Catalyst |
ACC QSil 940 QSI Quantum Silicones 40 Durometer Condensation Cure for Potting QSil 940 is a special purpose, two-component condensation cure siloxane elastomer that exhibits excellent release properties unless a primer is used which results in excellent adhesion. The material.. |
|||
Viscosity | 650 - 950 cP @Temperature 25.0 °C |
650 - 950 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PA-22 MDI Isocyanate Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyether-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for .. |