Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 550000 cP | 550000 cP | |
Ritelok PS67 Adhesive Anaerobic. Pipe sealant, standard and stainless pipes. PS67 withstands temperatures from 65°F to 400°F (55°C-200°C), dismantled using normal tools |
|||
Viscosity | 550000 cP @Temperature 400 °C |
550000 cP @Temperature 752 °F |
melt; ISO 11443 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Viscosity | 550000 cP @Temperature 400 °C |
550000 cP @Temperature 752 °F |
ISO 11443 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Viscosity | 550000 cP @Temperature 400 °C |
550000 cP @Temperature 752 °F |
Melt; ISO 11443 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Viscosity | 550000 cP @Shear Rate 190 1/s, Temperature 230 °C |
550000 cP @Shear Rate 190 1/s, Temperature 446 °F |
|
Noltex Soarnol® ET3808 Ethylene Vinyl Alcohol Copolymer Ethylene content 38 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Viscosity | 550000 cP @Temperature 180 °C |
550000 cP @Temperature 356 °F |
Melt; Flowtester (100 kgf/cm², dimension of die 1 Φ mm x 10 mm) |
Zeon Chemicals Quintac® 3421 SIS Block Polymer Styrene Isoprene (SIS) Block Polymer. Standard grade for hot melt PSAInformation provided by Zeon Chemicals L.P. |
|||
Viscosity | 550000 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
550000 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F128 PA6 Film Extrusion, Medium Viscosity |
|||
Viscosity | 550000 cP @Shear Rate 300 1/s, Temperature 190 °C |
550000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2090 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Viscosity | 550000 cP @Shear Rate 300 1/s, Temperature 190 °C |
550000 cP @Shear Rate 300 1/s, Temperature 374 °F |
ASTM D3835 |
Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
Viscosity | 550000 cP | 550000 cP | Part B, RVT, #7, 2.5 rpm; TM R050-12 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |