Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 50 - 100 cP @Temperature 25.0 °C |
50 - 100 cP @Temperature 77.0 °F |
Uncured |
Resin Technology Group UV-408 Low-Viscosity, High Clarity, UV Curable Adhesive UV 408 is a low viscosity, high clarity, UV curing adhesive with excellent adhesion to glass. The product is well suited for bonding close fitting parts and has excellent moisture resistance.Applica.. |
|||
Viscosity | 50 - 350 cP | 50 - 350 cP | |
Huntsman HY 5200 Aromatic Amine Approx. H+ equivalent weight 45. Mix Ratio with GY 6010 is 23.Comments/Applications: Liquid aromatic amine.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by H.. |
|||
Viscosity | 50 cP @Temperature 20.0 °C |
50 cP @Temperature 68.0 °F |
|
KiON CERASET® POLYUREASILIZANE 20 (PURS 20) General DescriptionKiON Ceraset Polyureasilazane is a liquid polymer that can easily be converted to a solid pre-ceramic and then be pyrolyzed to either silicon carbide or silicon nitride-containing.. |
|||
Viscosity | 50 cP | 50 cP | B-type viscometer (60rpm) |
Mitsui UNISTOLEâ„¢ R-200X Polyolefinic Primer/ Adhesive UNISTOLEâ„¢ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristi.. |
|||
Viscosity | 50 cP @Temperature 25.0 °C |
50 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 50 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | 50 cP | 50 cP | |
Solvay AG-RHOâ„¢ FM 3896 Surfactant Description: Agricultural Foam Marker Concentrate. Very low alcohol content. Performs well in hard water up to 1000 ppmChemical Name: FOAM MARKER CONCENTRATE CAS: 111-76-2, 64-17-5 Solubility in Wat.. |
|||
Viscosity | 50 - 350 cP | 50 - 350 cP | #2 SP at 60 rpm; 540MA3C56 |
Solvay MIRAPOL® SURF-S 480PF Surfactant Description: Rinse aid polymer specially formulated for auto dish wash powders, tablets and liquids. Phosphate-free. Recommended as a substitute to rinse aid surfactants. Enables raw material cost s.. |
|||
Viscosity | 50 - 200 cP | 50 - 200 cP | #2 sp @ 30 rpm; RP-0596 |
Solvay RHODOLINE® 286N Surfactant Description: Hydrophilic copolymer dispersant. Semi gloss to high gloss, TiO2 slurry, interior/exterior, low foam.Identification: AMMONIUM POLYACRYLATE COPOLYMER SOLUTIONAvailable in: North AmericaA.. |
|||
Viscosity | 50 - 150 cP | 50 - 150 cP | Part B |
Master Bond MasterSil 151Med Medical Grade Silicone Potting Compound Description: Master Bond MasterSil 151Med is a two component, low viscosity silicone compound for high performance potting and encapsulation. MasterSil 151Med is an addition cured system and does no.. |
|||
Viscosity | 50 cP @Temperature 200 °C |
50 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3220 Polyester, Flake Adhesive agent, Resin modifier, Soft type, Standard resinUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as a.. |
|||
Viscosity | <= 50 cP | <= 50 cP | Hardener |
Von Roll Isola IMI Varnish 74010A Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 19°C. Average solids: 60%. Usage Notes: Use with IMI 74010 hardener for final coat over field coils, windings, and heavy duty motors. |
|||
Viscosity | 50 cP | 50 cP | |
Dow PAPI™ 94 Polymeric MDI PAPI™ 901 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This products low viscosity, low functionality, increased diphenylmethane diisocyanate content and increased perc.. |
|||
Viscosity | 50 cP | 50 cP | |
BASF Lupranate® TF2115 Isocyanate Description: Lupranate® TF2115 Isocyanate is a low viscosity polymeric diphenylmethane diisocyanate (polymeric-MDI) enriched with monomeric-MDI.Information provided by BASF |
|||
Viscosity | 50 - 200 cP | 50 - 200 cP | |
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive 3M™ Scotch-Weld™ Non-Metallic Filled is a non-metal filled version of Scotch-Weld adhesive 2214 regular. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a pa.. |
|||
Viscosity | 50 cP | 50 cP | B Component; ASTM D1824 |
Aptek 2100-A/B Urethane Encapsulant and/or Potting Compound General purpose encapsulant and potting compound. Outstanding hydrolytic stability. Excellent adhesion to components/circuit boards. Low modulus, low stress. Field proven for military and space appl.. |
|||
Viscosity | 50 - 200 cP | 50 - 200 cP | |
Beijing Ranger Chem SM-828EK85 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 50 cP | 50 cP | |
3M P595 Teak & Glass Primer 3M™ Adhesion Promoter AP596 and 3M™ Primers P590, P591, P592, P595 and P597 are low viscosity adhesion promoters recommended for use with the 3M™ 500-Series Polyurethane Adhesives/Sealants and 3M.. |
|||
Viscosity | 50 - 200 cP | 50 - 200 cP | |
Beijing Ranger Chem SM-828X80 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 50 - 300 cP | 50 - 300 cP | RP-0596 |
Solvay RHODAPON® SB-8208/S STD Surfactant Description: Rhodapon® LX-28/AF3 is Sodium Lauryl Sulfate solution based on narrow-cut primary natural alcohol. This grade is preserved with Formalin. It provides excellent detergency, cleansing an.. |
|||
Viscosity | 50 cP | 50 cP | B-type viscometer (60rpm) |
Mitsui UNISTOLE™ R-200 Polyolefinic Primer/ Adhesive UNISTOLE™ R is a modified polyolefin dispersed in hydrocarbon-based solvent used as an adhesive for bonding metals to polyolefins. This can also be used as a metal coating agent. Characteristics E.. |
|||
Viscosity | 50 cP | 50 cP | |
KKPC KOSYN KSL 5153 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 5000 series has uniform, spherical, light, and hard granules made by polymerization of polystyrene. It was developed in order to improve gloss, whit.. |