Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 3300 cP @Temperature 25.0 °C |
3300 cP @Temperature 77.0 °F |
Uncured |
Resin Technology Group CT-523LV Cationic UV Cure Epoxy Adhesive CT-523-LV is an epoxy-based, low viscosity, cationic-curable adhesive and/or sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical re.. |
|||
Viscosity | 3300 - 4100 cP | 3300 - 4100 cP | |
Huntsman Araldite GY 282 Bisphenol F Epoxy Resin Weight per Epoxide (EEW, g/eq) 166 to 176. Max color is 5.Comments/Applications: Used in coatings, adhesives, tank linings, flooring, filament winding, casting pultrusion and RTM. Better chemical .. |
|||
Viscosity | 3300 cP @Shear Rate 50.0 1/s, Temperature 240 °C |
3300 cP @Shear Rate 50.0 1/s, Temperature 464 °F |
Melt; ASTM D3835 |
Kureha KF Polymer 1100 PVDF Homopolymer KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF p.. |
|||
Viscosity | 3300 cP | 3300 cP | Mixed (cp #40, 2.5 rpm) |
Tra-Con Tra-Bond 526M05 Rapid Low Temperature Cure Adhesive TRA-BOND 526M05 is a low viscosity, fast cure at low temperature, long pot-life adhesive. Information provided by Tra-Con Inc. |
|||
Viscosity | 3300 cP | 3300 cP | dynamic |
Dow Corning SLYGARD® 3-6636 SILICONE DIELECTRIC GEL KIT Two-part, transparent, LED encapsulant which is a lower-viscosity version of EG-6301.Information provided by Dow Corning |
|||
Viscosity | 3300 cP @Temperature -20.0 °C |
3300 cP @Temperature -4.00 °F |
Cold Crank |
ChevronTexaco 220R Neutral Oil FeaturesChevron Neutral Oils are all-hydroprocessed, highly refined API Group II paraffinic base stocks. Their extremely low sulfur, nitrogen, and aromatic content give them excellent thermal and o.. |
|||
Viscosity | 3300 - 4300 cP @Temperature 25.0 °C |
3300 - 4300 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PA-08 MDI Isocyanate Description of product: 4,4`-diphenyl-methane-diisocyanate and polyether-diol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for producing e.. |