Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 275 cP @Temperature 40.0 °C |
275 cP @Temperature 104 °F |
25% in dimethylacetamide; Internal Method |
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be g.. |
|||
Viscosity | 275 cP @Temperature 85.0 °C |
275 cP @Temperature 185 °F |
|
Northstar Polymers MSA-030 Polyester Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 275 cP | 275 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3600P Polyethersulfone (PESU) Veradel® PESU was formerly marketed as Gafone™ PESU. Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They ca.. |
|||
Viscosity | 275 cP | 275 cP | Part B |
Resinlab® UR3010 Black Polyurethane Potting System Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |
|||
Viscosity | 275 cP | 275 cP | Part B |
Resinlab® UR3010 Clear Polyurethane Potting System Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro.. |
|||
Viscosity | 275 cP | 275 cP | Liquid Property |
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)
(discontinued **) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |