Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 260000 cP @Temperature 25.0 °C |
260000 cP @Temperature 77.0 °F |
Uncured |
Permabond LH054 Anaerobic Threadsealant Permabond® LH054 is an anaerobic curing, calibrated strength pipe sealant that allows for easier disassembly – especially of larger diameter pipes. It cures anaerobically when in contact with meta.. |
|||
Viscosity | 260000 cP @Temperature 25.0 °C |
260000 cP @Temperature 77.0 °F |
Uncured |
Permabond LH150 Anaerobic Threadsealant Permabond® LH150 Pipe Sealant with PTFE is designed for sealing and locking tapered metal pipe threads and fittings. It is ideal for stainless steel and other passive metals. Instant sealing of up .. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® 359 PBT (Europe-Africa-Middle East) VALOX 359 is an unreinforced, flame retarded, low warpage PBT injection moulding resin. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
Viscosity | <= 260000 cP | <= 260000 cP | (Haake RU 20, 115 OSC, PK 2-1, 0; D= 1s<sup>-1</sup>) |
Dow BETAMATE™ 7200 Polyurethane Prepolymer BETAMATE™ 7200 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Viscosity | <= 260000 cP | <= 260000 cP | (Haake RU 20, 115 OSC, PK 2-1, 0; D= 1s<sup>-1</sup>) |
Dow BETAMATE™ 7201 Polyurethane Prepolymer BETAMATE™ 7201 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Viscosity | <= 260000 cP | <= 260000 cP | (Haake RU 20, 115 OSC, PK 2-1, 0; D= 1s<sup>-1</sup>) |
Dow BETAMATE™ 7205 Polyurethane Prepolymer BETAMATE™ 7205 is a one component moisture curing polyurethane seam sealant with permanent elasticity and good adhesion to different substrates. It is an excellent seam sealer for body repair. It.. |
|||
Viscosity | 260000 cP @Temperature 250 °C |
260000 cP @Temperature 482 °F |
DAM; @ 1000 sec-1; ISO 11443 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® V3900WX PBT+PC (Europe-Africa-Middle East) PBT/PC blend - Unreinforced - Flame Retardant. This is a UV-stabilized grade designed for outdoor enclosure applications requiring UL 746C F1 weatherability performance. |
|||
Viscosity | 260000 cP | 260000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |