Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.50e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
2.50e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Viscosity | 2.50e+6 cP @Shear Rate 50.0 1/s, Temperature 190 °C |
2.50e+6 cP @Shear Rate 50.0 1/s, Temperature 374 °F |
estimated from log-log graph |
DuPont Bynel® 4208 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Viscosity | 2.50e+6 cP @Temperature 25.0 °C |
2.50e+6 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Eccobond® C429-2 One-Component Silver Filled Electrically Conductive Epoxy Adhesive Emerson & Cuming C429-2 Eccobond® One-Component Silver Filled Electrically Conductive Epoxy AdhesiveOne component, high strength, moderate cost, silver filled, electrically conductive, epoxy adhesi.. |
|||
Viscosity | 2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F136 PA6 Very High Viscosity, Film Extrusion |
|||
Viscosity | 2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F136-C PA6 Film Extrusion, Very High Viscosity, Lubricated |
|||
Viscosity | 2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F136-C1 PA6 Very High Viscosity, Film Extrusion, Lubricated |
|||
Viscosity | 2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F136-E1 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity | 2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 260 °C |
2.50e+6 cP @Shear Rate 0.100 1/s, Temperature 500 °F |
|
DSM Akulon® F136-E2 PA6 Very High Viscosity, Lubricated, Nucleated, Film Extrusion |
|||
Viscosity | 2.50e+6 cP @Shear Rate 200 1/s, Temperature 190 °C |
2.50e+6 cP @Shear Rate 200 1/s, Temperature 374 °F |
Capillary viscosimeter |
BorsodChem ONGRO CPE 3602 C Chlorinated Polyethylene IMPACT MODIFIER FOR PVChigh impact resistancegood processabilityexcellent weather resistanceELASTOMERSvariety of cross-linking technologiesexcellent ozone- and weather resistanceexcellent chemical r.. |