Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 100 - 500 cP | 100 - 500 cP | |
ND Industries 530 Shaft & Bearing Retainer Retaining Compound General DescriptionA high strength adhesive for retention of cylindrical components, where disassembly is not required.Typical Usesrotors, shafts, bushings, bearings, and pulleysMeets military spec .. |
|||
Viscosity | 100 - 200 cP | 100 - 200 cP | |
ND Industries 600 Methacrylate Resin Activator Activator for structural Adhesives and anaerobics. Solvent free. |
|||
Viscosity | 100 cP | 100 cP | |
Parker Chomerics CHO-SHIELD® 4968 Silicone Coating Silicone Coating. This is a two-component silicone polymer system used to protect electronic components and assemblies against moisture, abrasion, dust, and chemicals. It is particularly intended to.. |
|||
Viscosity | 100 cP | 100 cP | |
Resinlab® CYNERGY CA6602 Adhesive Description: The CYNERGY 6600 SERIES are modified to provide greatly reduced odor and frosting of plastics. These products are ideal for bonding dissimilar materials with excellent performance on a .. |
|||
Viscosity | 100 - 110 cP | 100 - 110 cP | |
Huntsman DT 3126-2 Epoxy Accelerator Comments/Applications: Granular solid. Powder coating accelerator for epoxy/COOH functional polyesters, used at 2-3% levels.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has be.. |
|||
Viscosity | 100 cP | 100 cP | |
Hybrid Plastics FireQuench® PM 1287 Resin FireQuench® PM1287 is an optically transparent, fire retardant hybrid nanocomposite resin that can serve as a replacement for standard epoxy-vinyl ester and related resins. It can be employed as .. |
|||
Viscosity | <= 100 cP | <= 100 cP | |
KKPC KOSYN KSL 361 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 300 series is a Styrene-Butadiene Latex.Applications: Oil-resistant Foam Rubber, For Impregnation of Tire and Belt Cord, Foam Backing of Textile Goo.. |
|||
Viscosity | 100 - 140 cP | 100 - 140 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1162 P (SIS) Linear Triblock Copolymer Description: Kraton D1162 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 43%. It is supplied from North America in the physical form identified: .. |
|||
Viscosity | 100 - 250 cP | 100 - 250 cP | As Supplied |
Heraeus Cleviosâ„¢ P HC V4 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P HC V4 is an antistatic material based on PED.. |
|||
Viscosity | <= 100 cP | <= 100 cP | |
Solvay AG-RHOâ„¢ GPA Surfactant Description: Ag-RHO GPA is a surfactant for pesticide formulations. It is a bioactivator that can be used to replace alky polyglucosides (APG's) in aqueous formulations, tank mix adjuvants, and liqu.. |
|||
Viscosity | <= 100 cP | <= 100 cP | Cannon Fenske at 40°C; RPG62 |
Solvay GEROPON® T/36 DF Surfactant Identification: SODIUM POLYCARBOXYLATE, AQUEOUS SOLUTION. Solubility: Soluble in water. Insoluble in polar and aromatics solvents.Available in: Asia Pacific, Europe, Latin America and North AmericaA.. |
|||
Viscosity | 100 - 200 cP | 100 - 200 cP | Part B |
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea.. |
|||
Viscosity | 100 - 110 cP | 100 - 110 cP | mixed compound; thixotropic |
Master Bond MB250NT Low viscosity ethyl cyanoacrylate Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi.. |
|||
Viscosity | 100 cP | 100 cP | dynamic |
Dow Corning CE-8170 AF MICROEMULSION A microemulsion of a high molecular weight aminofunctional silicone polymer for use in hair care applications.Information provided by Dow Corning |
|||
Viscosity | 100 cP | 100 cP | dynamic |
Dow Corning SYL-OFF® SL 8 CROSSLINKER Solvent-free, fast curing, actively reduces mist at high speeds, good balance of cure and anchorage performanceInformation provided by Dow Corning |
|||
Viscosity | 100 cP | 100 cP | |
Elmer's Products Aron Alpha® 402X Cyanoacrylate Adhesive (Industrial Krazy Glue™) Engineered for high temperature and high impact resistance.Medium gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Poor on porous substrates. .. |
|||
Viscosity | 100 - 400 cP | 100 - 400 cP | |
Abatron BestBond® Waterborne Polyurethane Adhesive for Wood BestBond® is a versatile adhesive designed for both interior and exterior wood projects. BestBond® is water-resistant, easy to clean up, non-toxic, and flexible. Primary suggested uses include fur.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT BLUE |
ACC QM 107 QSI Quantum Silicones 7 Durometer Condensation Cure Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is us.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT PURPLE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT BLUE |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT PURPLE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Viscosity | 100 cP | 100 cP | Uncatalyzed, QM CAT BLUE |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Viscosity | <= 100 cP | <= 100 cP | |
3M Dynamar™ RC 5105 Rubber Curative 3M™ Dynamar™ Rubber Curatives RC 5105, RC 5110, RC 5115, RC 5120 and RC 5125 are liquid curatives that offer fast and easy incorporation into solvent based FKM solution coatings. RC 5105 is 70% bi.. |
|||
Viscosity | <= 100 cP | <= 100 cP | |
3M Dynamar™ RC 5125 Rubber Curative 3M™ Dynamar™ Rubber Curatives RC 5105, RC 5110, RC 5115, RC 5120 and RC 5125 are liquid curatives that offer fast and easy incorporation into solvent based FKM solution coatings. RC 5125 is a sila.. |
|||
Viscosity | 100 - 300 cP | 100 - 300 cP | #2 sp @ 30 rpm; RP-0596 |
Solvay RHODOLINE® 270 Surfactant Description: Polyacid dispersant. Highly versatile, economical and low foam, flat to gloss, ideal for interior application.Identification: ACRYLIC POLYMERCAS: 9003-04-7Available in: North America IR.. |
|||
Viscosity | 100 cP | 100 cP | |
KKPC KOSYN KSL 106 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 100 series are carboxy metamorphic styrene-butadiene latexes. They have a soft touch and high adhesive force.Applications: Carpet Backing, Adhesive .. |
|||
Viscosity | <= 100 cP | <= 100 cP | RP-0596 |
Solvay RHODAPON® UB-STD Surfactant Chemical Name: SODIUM LAUREL SULFATECAS: 68585-47-7 Available in: Asia Pacific, Europe, Latin America and North America Applications: RHODAPON® UB-STD is a primary anionic surfactant for emulsion p.. |