Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2300 - 3800 cP | 2300 - 3800 cP | |
ND Industries Toughened Ethyl SuperGlue 310 Black flexible Cyanoacrylate for metal, rubber, and plastic |
|||
Viscosity | 2800 - 3800 cP @Temperature 23.0 °C |