Polymer Property : Viscosity = 2800 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2300 - 2800 cP
2300 - 2800 cP
ND Industries SuperGlue Ethyl 322
High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III
Viscosity 1800 - 2800 cP

@Temperature 23.0 °C
1800 - 2800 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping
Product Description: EPO-TEK® H20S is a modified version of EPO-TEK® H20E, designed primarily for die stamping and dispensing techniques for chip bonding. EPO-TEK®H20S is a highly reliable, two ..
Viscosity 1800 - 2800 cP

@Temperature 23.0 °C
1800 - 2800 cP

@Temperature 73.4 °F
100 rpm
Epoxy Technology EPO-TEK® H20E-LV Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-LV is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a ..