Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 900 - 1500 cP | 900 - 1500 cP | |
ND Industries 541 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, cams, collars, flywheels, rotors to shaft |
|||
Viscosity | 900 - 1300 cP @Temperature 30.0 °C |
900 - 1300 cP @Temperature 86.0 °F |
|
Prodways PLASTCure Rigid 10 500 3D Printing Polymer Superior thermo-mechanical properties.Suitable for the manufacture of parts that require thermal stability, extreme accuracy and quick turnaround. Exceptional for parts that are designed for wind tu.. |
|||
Viscosity | 900 - 1200 cP | 900 - 1200 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 160 (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 900 - 1100 cP | 900 - 1100 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 160 LOW ODOR/LOW BLOOM (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 900 - 1200 cP | 900 - 1200 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 160SI Surface Insensitive (1000 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 160SI SURFACE INSENSITIVE advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Viscosity | 900 cP @Temperature 82.2 °C |
900 cP @Temperature 180 °F |
|
Northstar Polymers MGA-048 Polyether Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 900 cP @Temperature 25.0 °C |
900 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-044 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 900 - 1300 cP | 900 - 1300 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 45-40/11S Polycaprolactone based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: ShoeInformation provided by Merquinsa |
|||
Viscosity | 900 cP | 900 cP | Fed Std Method 4287 |
Humiseal 1A27LSE Urethane Conformal Coating Humiseal 1A27LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingPasses thermal shock test (MIL-I-46058C).. |
|||
Viscosity | 900 - 1500 cP | 900 - 1500 cP | |
Huntsman Araldite ECN 1400 Water-Based Adhesive/Coating Base Resin is ECN 1299. Typical Solids Content 40%. Mean Particle Size 4µm. Weight per Epoxide (EEW, g/eq), solids basis, 220 to 250.Comments/Applications: Adhesives; Fiber-Sizing; Textiles; A.. |
|||
Viscosity | 900 - 1300 cP | 900 - 1300 cP | |
Huntsman Araldite GZ 7071 OX-65 Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 455 to 525. Max color is 2.Comments/Applications: GT 7071 - 65% solids in Aromatic 100 (13%) and xylene (22%) High performance 2-package systems for coatings, floorin.. |
|||
Viscosity | 900 - 2400 cP | 900 - 2400 cP | |
Huntsman HY 3100 Aromatic Amine Approx. H+ equivalent weight 55. Mix Ratio with GY 6010 is 23.Comments/Applications: High solids coatings, floorings and tank linings. Good acetic acid resistance and other aggressive environment.. |
|||
Viscosity | 900 - 1700 cP | 900 - 1700 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1161 J (SIS) Linear Triblock Copolymer Description: Kraton D1161 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t.. |
|||
Viscosity | 900 cP | 900 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1163 P (SIS) Linear Triblock Copolymer Description: Kraton D1163 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:.. |
|||
Viscosity | 900 - 1300 cP | 900 - 1300 cP | 15% Toluene Solution at 25°C; KM 06 |
Kraton® D1184 K (SBS) Branched Triblock Copolymer Description: Kraton D1184 K is a clear, branched triblock copolymer based on styrene and butadiene, with a polystyrene content of 31%. It is supplied from North America in the physical form indentif.. |
|||
Viscosity | 900 - 1500 cP | 900 - 1500 cP | 20% Toluene Solution at 25°C; BAM 922 |
Kraton® G1660 H (SEBS) Linear Triblock Copolymer Description: Kraton G1660 H is a linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 31%. It is supplied from North America in the physical form identified.. |
|||
Viscosity | 900 - 1100 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
900 - 1100 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2081126P2 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electrochemical sensors and conductive tracks. It may be .. |
|||
Viscosity | 900 - 1500 cP | 900 - 1500 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1102 A (SBS) Liner Block Copolymer Description: Kraton D1102 A is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 29.5% mass. It is supplied from Europe in the physical form(s) identified below in.. |
|||
Viscosity | 900 cP @Temperature 25.0 °C |
900 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8120 Silicone Stabilizer for PU Foam STRUKSILON 8120 was developed as universal silicone stabilizer of high potency for the production of conventional as well as flame retardant flexible polyurethane slabstock foam based on polyether p.. |
|||
Viscosity | 900 cP | 900 cP | Before Curing |
Silikony Polskie Polastosil M-99 Silicone Rubber Rubber with strong hardness |
|||
Viscosity | 900 cP @Temperature 25.0 °C |
900 cP @Temperature 77.0 °F |
|
Struktol STRUKSILON 8018 Silicone Stabilizer for PU-Microcellular Foam STRUKSILON 8018 is used as a silicone stabilizer for the production of polyurethane microcellular foam. It is especially recommended for shoe sole formulations based on polyester and blends of polye.. |
|||
Viscosity | 900 cP | 900 cP | |
Von Roll Isola IMI Varnish 716 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 56°C. Usag.. |
|||
Viscosity | 900 cP | 900 cP | LVT, sp2, 65 pm |
Dow Corning 1500 Antifoam 100% active silicone fluid containing a suspension of finely powdered silica to enhance its defoaming efficiency. Food grade antifoam.Information provided by Dow Corning |
|||
Viscosity | 900 cP | 900 cP | Uncatalyzed, QM 260B |
ACC QM 260 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 260 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Viscosity | 900 cP @Temperature 25.0 °C |
900 cP @Temperature 77.0 °F |
at 100/14 (50-6/50-12) pbw |
Abatron AboCast 50-6/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Colorless. Shelf life is 12+ months. |
|||
Viscosity | 900 - 1100 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
900 - 1100 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080415D2 Silver Counter Electrode Paste This product is a screen printable polymer paste designed as a counter electrode in electrochemical biosensors. This ink can be used in conjunction with our working carbon electrode ink C2030519P4, .. |
|||
Viscosity | 900 - 1400 cP | 900 - 1400 cP | #3 SP @ 60 rpm; RP-0596 |
Solvay RHODOLINE® 640 Surfactant Description: Mineral oil based defoamers for flat to gloss paints, great process foam know down.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 640 is a hydroph.. |
|||
Viscosity | 900 - 1500 cP @Temperature 25.0 °C |
900 - 1500 cP @Temperature 77.0 °F |
Uncured |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |