Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 800 - 1300 cP @Temperature 25.0 °C |
800 - 1300 cP @Temperature 77.0 °F |
|
Northstar Polymers MPC-022 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1200 cP @Temperature 25.0 °C |
800 - 1200 cP @Temperature 77.0 °F |
|
Northstar Polymers PAA-071 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1400 cP @Temperature 71.1 °C |
800 - 1400 cP @Temperature 160 °F |
|
Northstar Polymers SBX-146 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1500 cP @Temperature 23.9 °C |
800 - 1500 cP @Temperature 75.0 °F |
|
TSE Industries EcoWIND® 200 Polyurethane Resin Filament Winding
(discontinued **) TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 800 - 2300 cP | 800 - 2300 cP | |
Huntsman HZ 815 X-70 US Aromatic Amine Approx. H+ equivalent weight 150. Mix Ratio with GY 6010 is 81.Comments/Applications: Solution of HY 815, 70% solids in xylene. Trade sale paint enamels. Industrial maintenance, FDA. Flexible m.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-632L TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 800 cP | 800 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Virantage® VW-10200 RP, RFP, RSFP Polyethersulfone (PESU) Virantage® VW-series functionalized polyethersulfones (r-PESU) are amorphous, high-temperature sulfone polymers featuring reactive end groups to enhance solubility and improve interfacial propert.. |
|||
Viscosity | 800 cP | 800 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Virantage® VW-10300 P, FP & SFP Polyethersulfone (PESU) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Three grades are offered: Virantage® VW-10300P, Virantage® VW-10300FP, and Vira.. |
|||
Viscosity | 800 cP @Temperature 23.0 °C |
800 cP @Temperature 73.4 °F |
|
Master Bond EP29LP Low Exotherm, Low Viscosity Two Component Epoxy System Master Bond Polymer System EP29LP is a two component high performance epoxy resin system featuring low viscosity, long pot life and low exotherm. As an adhesive this versatile material will form bon.. |
|||
Viscosity | 800 cP | 800 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 6 Crosslinker Minimizes mist at speeds up to 1600 m/min, good balance of cure and anchorage performance.Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning SYL-OFF® SL 10 RELEASE MODIFIER Olefin-free; low viscosityInformation provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning SYL-OFF® SL 50 RELEASE MODIFIER Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | dynamic |
Dow Corning SYL-OFF® SL 6 CROSSLINKER Minimizes mist at speeds up to 1600 m/min, good balance of cure and anchorage performance.Information provided by Dow Corning |
|||
Viscosity | 800 cP | 800 cP | |
Elmer's Products Aron Alpha® 282F Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Viscosity | 800 - 1200 cP | 800 - 1200 cP | |
Epoxyset Epoxibond EB-119M Unfilled Epoxy Adhesive A two-component,unfilled, low viscosity, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by.. |
|||
Viscosity | 800 cP | 800 cP | |
ACC EP MAP-14 EPI Engineered Polymers Aliphatic Polymer EP MAP, “Powered by Reactamine® Technology”, are modified aliphatic prepolymers with monomer-extracted levels of a maximum of 0.2%. The polymers are made from HDI. EP MAP-14 contains 14% NCO. Pa.. |
|||
Viscosity | 800 cP | 800 cP | |
Abatron AboCast 8503-3/AboCure 8503-3 Colorless Epoxy AboCast 8503-3/AboCure 8503-3 is a general purpose, medium speed, colorless epoxy casting compound with low viscosity. It has a good balance of properties with a fairly fast hardening. Suggested Use.. |
|||
Viscosity | 800 - 1200 cP @Temperature 35.0 °C |
800 - 1200 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 05 Low Viscosity Polymeric Plasticizer Description: Used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 800 cP | 800 cP | A Side |
ACC EP RSP EPI Engineered Polymers Silicone Polyurea EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time.. |
|||
Viscosity | 800 cP | 800 cP | Side A |
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti.. |
|||
Viscosity | 800 - 1000 cP | 800 - 1000 cP | |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Viscosity | 800 cP | 800 cP | |
Von Roll Isola IMI Varnish 702 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 46°C. Usag.. |
|||
Viscosity | 800 cP @Temperature 40.0 °C |
800 cP @Temperature 104 °F |
25% solution in DMAc; Internal Method |
Solvay Specialty Polymers Virantage® VW-10300 P, FP Polyethersulfone (PESU)
(Unverified Data**) Virantage® VW-10300 polyethersulfone (PESU) is a non-functionalized, high-temperature sulfone polymer powder. Two grades are offered: Virantage VW-10300P and Virantage VW-10300FP, providing two par.. |
|||
Viscosity | 800 - 1500 cP @Temperature 23.0 °C |
800 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7SP4 Low Shrinkage, One Component, UV Curable System Master Bond Polymer System UV15-7SP4 is a one component, low viscosity UV system with flexibility. UV15-7SP4 has very little shrinkage when curing and has non-yellowing properties. It bonds well to .. |
|||
Viscosity | 800 - 1500 cP @Temperature 23.0 °C |
800 - 1500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7SP4DC One Component, Dual Cured, Flexible UV System Master Bond Polymer System UV15-7SP4DC is a one component, optically clear, dual cured flexible UV and/or heat curable polymer system with extended service capability of -80°F to +250°F. It cures .. |
|||
Viscosity | 800 cP | 800 cP | |
KKPC KOSYN KSL 341 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 300 series is a Styrene-Butadiene Latex. KSL 341 has big granules and high concentration. It shows excellent processability in rubber sponge produc.. |