Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 65 cP @Temperature 30.0 °C |
65 cP @Temperature 86.0 °F |
15% wt, Toluene Solution |
Kuraray SEPTON® S4030 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Viscosity | 65 - 85 cP | 65 - 85 cP | |
Huntsman MT 0163 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 181 to 200.Comments/Applications: Solid tetra-functional phenol-based epoxy resin. Provides exceptional strength at elevated temperatures, as well as improved thermal.. |
|||
Viscosity | 65 cP @Temperature 25.0 °C |
65 cP @Temperature 77.0 °F |
Solution Viscosity in 5 wt.% Toluene; UBE Method |
UBE UBEPOL BR340L Non-Oil Extended Synthetic Rubber (Raw Polymer) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Microstructure: cis: 98trans: 1vinyl: 1Information provided by UBE. |
|||
Viscosity | 65 cP | 65 cP | |
BASF Lupranate® 78 Isocyanate Description: Lupranate® 78 Isocyanate is a polymeric MDI with a functionality of approximately 2.3. This product exhibits excellent low temperature stability. Lupranate 78 Isocyanate will remain a .. |
|||
Viscosity | 65 cP | 65 cP | B Component; Spindle #2; speed 100 rpm; ASTM D1824 |
Aptek 6110-A/B Epoxy Encapsulant and/or Potting Compound Optoelectronic grade encapsulant/potting compound – will not attack/cloud polysulphone casings. More flexible, lower Tg version of APTEK 6106-A/B, for good temperature cycling in ceramic devices.P.. |