Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 550 - 350000 cP | 550 - 350000 cP | Average value: 27500 cP Grade Count:27 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |
|||
Viscosity | 550 - 850 cP | 550 - 850 cP | |
Huntsman Euredur 43 S Cycloaliphatic Amine Approx. H+ equivalent weight 115. Mix Ratio with GY 6010 is 60.Comments/Applications: Euredur 43 S is the accelerated version of Euredur 43.Data provided by Ciba Specialty Chemicals.Ciba Specialty.. |
|||
Viscosity | 550 - 850 cP | 550 - 850 cP | |
Huntsman MY 0510 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 95 to 107. Color: BrownComments/Applications: High purity MY 0500. Improved stability. Boosts performance of bisphenol A resins. Used for rapid cure adhesives, lam.. |
|||
Viscosity | 550 - 850 cP @Temperature 125 °C |
550 - 850 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® N-35 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-35 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 550 cP @Temperature 30.0 °C |
550 cP @Temperature 86.0 °F |
|
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur.. |
|||
Viscosity | 550 - 750 cP | 550 - 750 cP | |
Dow CYRACURE™ UVR-6128 Cycloaliphatic Epoxide CYRACURE™ UVR-6107 cycloaliphatic epoxide is a standard flexibilizing cycloaliphatic epoxide resin. Typical applications include: Metal decoration coatings Overprint varnishes Flexible packaging .. |
|||
Viscosity | 550 cP | 550 cP | dynamic |
Dow Corning 3-4154 DIELECTRIC GEL KIT Two-part, clear, RT or heat cure.Information provided by Dow Corning |
|||
Viscosity | 550 - 700 cP @Temperature 35.0 °C |
550 - 700 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 70 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 550 - 800 cP @Temperature 35.0 °C |
550 - 800 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 72 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of conveyor belt manufacturing as well as in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 550 cP | 550 cP | B Side |
ACC EP RAP-1567 EPI Engineered Polymers Aliphatic Polyurea RAP-1567 HX is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generat.. |
|||
Viscosity | 550 cP | 550 cP | B Side |
ACC EP RAP-1567 HX EPI Engineered Polymers Aliphatic Polyurea RAP-1567 is a two component 100% solids, no VOC’s, aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This new generation.. |
|||
Viscosity | 550 cP | 550 cP | B Side |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This ne.. |
|||
Viscosity | 550 cP | 550 cP | B Side |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This.. |
|||
Viscosity | 550 - 750 cP | 550 - 750 cP | |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Viscosity | 550 cP | 550 cP | |
Abatron AboCast 50-3/AboCure 8110-1 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Viscosity | 550 cP | 550 cP | |
Dymax 3069 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |