Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 5.0 cP | 5.0 cP | |
ND Industries 621 Heptane-Acetone SuperGlue accelerator Fast acting SuperGlue accelerator 15 seconds. Non-ozone depleting but flammable solvent |
|||
Viscosity | 5.0 cP | 5.0 cP | |
ND Industries 623 Heptane-Acetone SuperGlue accelerator Fast Acting SuperGlue accelerator, general purpose for porous surfaces or large gaps. Non-ozone depleting but flammable solvent |
|||
Viscosity | 5.0 cP | 5.0 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 190 CLEAR FLEXIBLE (4000 Viscosity) Rapid Bonding Adhesive Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 120 LOW ODER advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's p.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6101 Adhesive Description: The CYNERGY 6100 SERIES products are used to bond metal to itself or other substrates. It is available in five standard viscosities.Application: The CYNERGY SERIES of the cyanoacrylates.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6201 Adhesive Description: The CYNERGY 6200 SERIES products are for use in demanding applications where very fast cure speeds are required. Also used when difficult to bond and acidic surfaces are used such as EP.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6301 Adhesive Description: The CYNERGY 6300 SERIES products are for use in applications where a faster set time is desired or low moisture conditions exist. Provides good bonds to a wide variety of materials.Appl.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6001 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6002 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6701 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Viscosity | 5.0 cP | 5.0 cP | |
Resinlab® CYNERGY CA6901 Adhesive Description: The CYNERGY 6900 SERIES are for use in demanding applications where very fast cure speeds and high temperature resistance are required. These are single component solvent free materials.. |
|||
Viscosity | 5.0 - 20 cP | 5.0 - 20 cP | As Supplied |
Heraeus Cleviosâ„¢ P Jet HC Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet HC is an antistatic material based on PE.. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
As Supplied |
Heraeus Cleviosâ„¢ P Jet HC V2 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet HC V2 is an antistatic material based on.. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
|
Heraeus Cleviosâ„¢ P Jet N Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ PT2 is an antistatic material based on PEDOT:P.. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
As Supplied |
Heraeus Cleviosâ„¢ P Jet N V2 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet N V2 is an antistatic material based on .. |
|||
Viscosity | 5.0 - 20 cP @Shear Rate 11.7 1/s |
5.0 - 20 cP @Shear Rate 11.7 1/s |
As Supplied |
Heraeus Cleviosâ„¢ P Jet UA Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P Jet UA is an antistatic material based on PE.. |
|||
Viscosity | 5.0 - 12 cP | 5.0 - 12 cP | As Supplied |
Heraeus Cleviosâ„¢ P VP AI 4083 Conductive Sulfonate Polymer for Antistatic Coatings Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Cleviosâ„¢ P VP AI 4083 is an antistatic material based o.. |
|||
Viscosity | 5.0 - 15 cP | 5.0 - 15 cP | ASTM D445 |
ExxonMobil Jayflex™ MB10 Plasticizer (European Grade) Availability: Europe, Middle East & AfricaCAS Number: 131298-44-7EINECS Number: 421-090-1Information provided by ExxonMobil |
|||
Viscosity | 5.0 cP @Temperature 20.0 °C |
5.0 cP @Temperature 68.0 °F |
|
Akzo Nobel Trigonox® 301 Polymerization Initiator Initiator for the production of controlled rheology polypropylene (CR-PP).Chemical description: 3,6,9-Triethyl-3,6,9-trimethyl-1,4,7-triperoxonane, 41% solution in isoparaffinic hydrocarbonsCAS Numb.. |
|||
Viscosity | <= 5.0 cP | <= 5.0 cP | |
3M Scotch-Weld™ AC68 Instant Adhesive Debonder 3M™ Scotch-Weld™ Instant Adhesive Debonder AC68 attacks and dissolves cured instant adhesives. It is formulated to have a relatively low evaporation rate and can be used to debond misaligned parts.. |
|||
Viscosity | <= 5.0 cP | <= 5.0 cP | |
3M Scotch-Weld™ AC78 Instant Adhesive Primer 3M™ Scotch-Weld™ Instant Adhesive Primer AC78 helps to bind elastomeric materials including silicone.Information provided by 3M |
|||
Viscosity | 5.0 cP | 5.0 cP | |
3M Scotch-Weld™ LO5 Low Odor Instant Adhesive 3M™ Scotch-Weld™ Low-Odor Instant Adhesives are formulated to have low volatility while maintaining bonding of a wide rage of materials. Low volatility means that these products are not only low o.. |
|||
Viscosity | <= 5.0 cP | <= 5.0 cP | |
3M Scotch-Weld™ MG79 AC Medical Grade Instant Adhesive Primer 3M™ Scotch-Weld™ Medical Grade Instant Adhesive Primers are liquid chemical products used in conjunction with 3M™ Scotch-Weld™ Medical Grade Instant Adhesives. MG 79 AC is a cyanoacrylate primer.. |
|||
Viscosity | <= 5.0 cP | <= 5.0 cP | |
3M Scotch-Weld™ AC09 Instant Adhesive Activator 3M™ Scotch-Weld™ Instant Adhesive Activator AC09 is a fluorinated solvent based activator that is non-flammable.Information provided by 3M |
|||
Viscosity | 5.0 cP @Temperature 25.0 °C |
5.0 cP @Temperature 77.0 °F |
|
Parker Chomerics CHO-SHIELD® 1085 Silicone Adhesive Primer Air-drying liquid coatings used to improve the adhesion of Chomerics CHO-BOND conductive silicone elastomers to metal and other non-silicone substrates. The primers are moisture reactive and clear i.. |
|||
Viscosity | 5.0 cP @Temperature 25.0 °C |
5.0 cP @Temperature 77.0 °F |
|
Parker Chomerics CHO-SHIELD® 1086 Silicone Adhesive Primer Air-drying liquid coatings used to improve the adhesion of Chomerics CHO-BOND conductive silicone elastomers to metal and other non-silicone substrates. The primers are moisture reactive and clear i.. |
|||
Viscosity | 5.0 cP @Temperature 25.0 °C |
5.0 cP @Temperature 77.0 °F |
|
Parker Chomerics CHO-SHIELD® 1091 PRIMER CHO-SHIELD 1091 is an air-drying liquid coating for enhancing the adhesion of CHO-SHIELD 2001 and 2003 corrosion resistant, electrically conductive coatings to chemically treated aluminum. CHO-SHIEL.. |